Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 3.90 kJ/m² @Temperature -40.0 °C |
1.86 ft-lb/in² @Temperature -40.0 °F |
ISO 180 |
Eastman Eastar GN125 Copolyester, Natural
(discontinued **) Eastar Copolyester GN125 is a glycol modified polyethylene terephthalate (PET) that contains an ultraviolet light inhibitor. This product is recommended for indoor applications requiring enhanced co.. |
|||
Izod Impact, Notched (ISO) | 3.90 kJ/m² @Temperature -40.0 °C |
1.86 ft-lb/in² @Temperature -40.0 °F |
ISO 180 |
Eastman 9921P PET Injection Molded
(discontinued **) Voridian PET 9921P is produced at Voridian’s manufacturing sites in Rotterdam and Zarate, it is PTA/CHDM based, and it is sold to customers in the Europe, Middle East and Africa, Argentina, Bolivia.. |
|||
Izod Impact, Notched (ISO) | 3.90 kJ/m² @Temperature -40.0 °C |
1.86 ft-lb/in² @Temperature -40.0 °F |
ISO 180 |
LyondellBasell Hifaxâ„¢ CA244 Thermoplastic Polyolefin Elastomer Description: Hifaxâ„¢ CA244 high melt flow, 850 MPa flexural modulus, paintable thermoplastic elastomeric olefin (TEO) resin has an excellent combination of stiffness, processability and dynamic.. |
|||
Izod Impact, Notched (ISO) | 3.90 kJ/m² @Temperature -30.0 °C |
1.86 ft-lb/in² @Temperature -22.0 °F |
ISO 180 |
LyondellBasell Hostacomâ„¢ CB275FC Thermoplastic Polyolefin Elastomer Description: Hostacomâ„¢ CB275FC high melt flow, 1,900 MPa flexural modulus, precolored, UV-stabilized, mineral-filled thermoplastic elastomeric olefin (TEO) resin has an excellent balance of pro.. |
|||
Izod Impact, Notched (ISO) | 3.90 kJ/m² @Temperature -40.0 °C |
1.86 ft-lb/in² @Temperature -40.0 °F |
ISO 180 |
BASF Ultramid® B3GM35 BK 60564 40% Glass/Mineral Filled PA6 (Dry) Description: Ultramid B3GM35 BK60564 is a 40% combined glass-fiber and mineral reinforced, pigmented black injection molding PA6 grade.Applications: industrial articles requiring medium rigidity and.. |