Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 49.0 kJ/m² @Temperature -30.0 °C |
23.3 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Lexan® ML7647 PC Non FR Impact modified PC, excellent Fatigue performance with balanced Flow and impact. Available in Opaque onlyThis data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched (ISO) | 49.0 kJ/m² @Temperature -30.0 °C |
23.3 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Lexan® ML7666 PC (Asia Pacific) Non FR Impact modified PC, excellent Fatigue performance with balanced Flow and impact. Available in Opaque onlyThis data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched (ISO) | 49.0 kJ/m² @Temperature 23.0 °C |
23.3 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Ultem UR9076LG PEI Standard flow mineral filled Polyetherimide Blend. Restricted sales to GE Specialty Film & Sheet.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched (ISO) | 49.0 kJ/m² @Temperature 23.0 °C |
23.3 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Xenoy® XD549S PBT+PC (Europe-Africa-Middle East) Xenoy XD549S is an automotive grade, designed for thin wall (2.5 mm.) direct gated exterior parts. The material has an excellent flow. Xenoy XD549S can be painted with primerless solvent or waterbas.. |