Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Four Ball Wear | 0.600 mm | 0.0236 in | Avg. scar diameter; ASTM D4172 |
Solvay Specialty Polymers FOMBLIN® LC08 PFPE Lubricant FOMBLIN LC perfluoropolyether fluids have the following unique features: excellent wear characteristics; very good low temperature properties; cost-effective; and outstanding for applications requir.. |
|||
Four Ball Wear | 0.600 mm | 0.0236 in | Avg. scar diameter; ASTM D4172 |
Solvay Specialty Polymers FOMBLIN® LC55 PFPE Lubricant FOMBLIN LC perfluoropolyether fluids have the following unique features: excellent wear characteristics; very good low temperature properties; cost-effective; and outstanding for applications requir.. |
|||
Four Ball Wear | 0.600 mm | 0.0236 in | Avg. scar diameter; ASTM D4172 |
Solvay Specialty Polymers FOMBLIN® LC80 PFPE Lubricant FOMBLIN LC perfluoropolyether fluids have the following unique features: excellent wear characteristics; very good low temperature properties; cost-effective; and outstanding for applications requir.. |
|||
Four Ball Wear | 0.600 mm | 0.0236 in | 40 kg, 1200 rpm; ASTM D2266 |
ExxonMobil Unirex S 2 Unirex S 2 is premium-quality high-temperature grease, based on a low volatility, synthetic polyol ester fluid, thickened with a lithium complex soap thickener, and containing performance-enhancing .. |
|||
Four Ball Wear | 0.600 mm | 0.0236 in | 40 kg, 1200 rpm, 75°C, 1 hr; ASTM D2266 |
ExxonMobil Mobil Polyrex EM 103 Super-premium Mobil Polyrex EM Series grease is specially formulated for electric-motor bearings. The advanced thickener formulation and proprietary manufacturing techniques provide improved bearing.. |
|||
Four Ball Wear | 0.600 mm | 0.0236 in | |
ChevronTexaco 100 NC Open Gear Lubricant FeaturesChevron Open Gear Lubricants are black, viscous lubricants formulated with an asphaltic base and diluted with a nonchlorinated solvent for easy application by hand or through automatic lubri.. |
|||
Four Ball Wear | 0.600 mm | 0.0236 in | |
ChevronTexaco 250 NC-HT Open Gear Lubricant FeaturesChevron Open Gear Lubricants are black, viscous lubricants formulated with an asphaltic base and diluted with a nonchlorinated solvent for easy application by hand or through automatic lubri.. |
|||
Four Ball Wear | 0.600 mm | 0.0236 in | |
ChevronTexaco NC Open Gear Grease FeaturesChevron Open Gear Greases are formulated with high viscosity mineral oils in a nonsoap-based thickener. These greases appear brownish-black and are extremely tacky.Chevron Open Gear Greases .. |
|||
Four Ball Wear | 0.600 mm | 0.0236 in | |
ChevronTexaco Open Gear Grease FeaturesChevron Open Gear Greases are formulated with high viscosity mineral oils in a nonsoap-based thickener. These greases appear brownish-black and are extremely tacky.Chevron Open Gear Greases .. |
|||
Four Ball Wear | 0.600 mm | 0.0236 in | Scar Diameter |
ChevronTexaco Polystar® CVJ Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.Notes:Minimum operating temperature is the lowest tempe.. |
|||
Four Ball Wear | 0.600 mm | 0.0236 in | 40 kg, 1200 rpm, 75°C, 1 hr; ASTM D2266 |
ExxonMobil Mobil Polyrex EM 103 Super-premium Mobil Polyrex EM Series grease is specially formulated for electric-motor bearings. The advanced thickener formulation and proprietary manufacturing techniques provide improved bearing.. |
|||
Four Ball Wear | 0.600 mm | 0.0236 in | 40 kg, 1200 rpm; ASTM D2266 |
ExxonMobil Unirex S 2 Unirex S 2 is premium-quality high-temperature grease, based on a low volatility, synthetic polyol ester fluid, thickened with a lithium complex soap thickener, and containing performance-enhancing .. |
|||
Four Ball Wear | 0.600 mm | 0.0236 in | 1 hr. @ 1200 rpm, 75°C (167°F), 40 kg.; ASTM D-2266 |
ConocoPhillips ANDEROL® 783-2 Series Synthetic Food Grade Greases, NLGI Grade 2 Description: ANDEROL 783 Series Greases are made from synthetic hydrocarbons (PAO) and an aluminum complex soap thickener, allowing for a wide range of operating temperatures. The 783 Series Greases.. |
|||
Four Ball Wear | 0.600 mm | 0.0236 in | 1 hr. @ 1200 rpm, 75°C (167°F), 40 kg.; ASTM D-4172 |
ConocoPhillips ANDEROL® FGC 150 Compressor Fluid, Synthetic Food Grade ISO 150 Description: ANDEROL FGC 150 Compressor Fluid is a synthetic hydrocarbon (PAO) based lubricant formulated with special additive packages that provide good thermal and oxidative stability to keep val.. |
|||
Four Ball Wear | 0.600 mm | 0.0236 in | 1 hr. @ 1200 rpm, 75°C (167°F), 40 kg.; ASTM D-4172 |
ConocoPhillips ANDEROL® FGC 20 Synthetic Food Grade Compressor Fluid, ISO 46 Description: ANDEROL FGC Series Compressor Fluids are synthetic hydrocarbon (PAO) based lubricants formulated for use in compressors. FGC Series Fluids meet the former H-1 approval requirements of t.. |
|||
Four Ball Wear | 0.600 mm | 0.0236 in | 1 hr. @ 1200 rpm, 75°C (167°F), 40 kg.; ASTM D-4172 |
ConocoPhillips ANDEROL® FGC 30 Synthetic Food Grade Compressor Fluid, ISO 68 Description: ANDEROL FGC Series Compressor Fluids are synthetic hydrocarbon (PAO) based lubricants formulated for use in compressors. FGC Series Fluids meet the former H-1 approval requirements of t.. |
|||
Four Ball Wear | 0.600 mm | 0.0236 in | 1 hr. @ 1200 rpm, 75°C (167°F), 40 kg.; ASTM D-4172 |
ConocoPhillips ANDEROL® FGC 40 Compressor Fluid, Synthetic Food Grade ISO 100 Description: ANDEROL FGC 40 Compressor Fluid is a synthetic hydrocarbon (PAO) based lubricant formulated for use in compressors. FGC 40 Fluid meets the former H-1 approval requirements of the USDA w.. |
|||
Four Ball Wear | 0.600 mm | 0.0236 in | 1 hr. @ 1200 rpm, 75°C (167°F), 40 kg.; ASTM D-4172 |
ConocoPhillips ANDEROL® FGC 5 Fluid, Synthetic Mechanical Seal Fluid ISO 22 Description: ANDEROL FGC 5 Mechanical Seal Fluid is a synthetic hydrocarbon (PAO) based lubricant. FGC 5 Fluid meets the former H-1 approval requirements of the USDA where incidental food contact ca.. |
|||
Four Ball Wear | 0.600 mm | 0.0236 in | |
ChevronTexaco Rykon® 1426 Premium Grease Chevron Rykon Premium Grease No. 1426 contains polyurea thickener, highly refined paraffinic base oil, rust and oxidation inhibiting additives, as well as heatstable extreme pressure additives.Appli.. |
|||
Four Ball Wear | 0.600 mm | 0.0236 in | 1 hr. @ 1200 rpm, 75°C (167°F), 40 kg.; ASTM D-4172 |
ConocoPhillips ANDEROL® FGC 10 Synthetic Food Grade Compressor Fluid, ISO 32 Description: ANDEROL FGC Series Compressor Fluids are synthetic hydrocarbon (PAO) based lubricants formulated for use in compressors. FGC Series Fluids meet the former H-1 approval requirements of t.. |
|||
Four Ball Wear | 0.600 mm | 0.0236 in | |
ConocoPhillips 2 Bentone Grease NLGI No. 2 Description: Conoco Bentone Grease is a high-quality, smooth-textured, clay based grease developed for heavy-duty industrial machinery operating at very high temperatures. Unlike conventional soap-b.. |
|||
Four Ball Wear | 0.600 mm | 0.0236 in | |
ChevronTexaco Aerosol Open Gear Grease FeaturesChevron Open Gear Greases are formulated with high viscosity mineral oils in a nonsoap-based thickener. These greases appear brownish-black and are extremely tacky.Chevron Open Gear Greases .. |