Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Four Ball Extreme Pressure, Weld Load | 250 kg | 551 lb (mass) | Welding Load; IP 239 |
Solvay Specialty Polymers FOMBLIN® LC08 PFPE Lubricant FOMBLIN LC perfluoropolyether fluids have the following unique features: excellent wear characteristics; very good low temperature properties; cost-effective; and outstanding for applications requir.. |
|||
Four Ball Extreme Pressure, Weld Load | 250 kg | 551 lb (mass) | ASTM D2596 |
ExxonMobil 0 Mobilux EP Mobilux EP 0, 1, 2, 3, and 023 products are a high performance family of five general-purpose industrial greases and two special-duty semi-fluid greases. These lithium hydroxystearate greases are fo.. |
|||
Four Ball Extreme Pressure, Weld Load | 250 kg | 551 lb (mass) | ASTM D2596 |
ExxonMobil 1 Mobilith AW Series The Mobilith AW Series products are high performance lithium-complex greases. They are formulated with antiwear agents to provide excellent service under the severe operating conditions of heavy and.. |
|||
Four Ball Extreme Pressure, Weld Load | 250 kg | 551 lb (mass) | ASTM D2783 |
ExxonMobil 1000 Mobilgear SHC Series The Mobilgear SHC Series lubricants are heavy-duty gear oils primarily designed for all kinds of enclosed gearing as well as plain and rolling element bearings. They are formulated from wax-free pol.. |
|||
Four Ball Extreme Pressure, Weld Load | 250 kg | 551 lb (mass) | ASTM D2596 |
ExxonMobil 220 Mobilith SHC Series Mobilith SHC Series greases are supreme performance products designed for a wide variety of applications at extremes of temperature. They combine the unique features of synthetic base fluids with th.. |
|||
Four Ball Extreme Pressure, Weld Load | 250 kg | 551 lb (mass) | ASTM D2596 |
ExxonMobil 3 Mobilith AW Series The Mobilith AW Series products are high performance lithium-complex greases. They are formulated with antiwear agents to provide excellent service under the severe operating conditions of heavy and.. |
|||
Four Ball Extreme Pressure, Weld Load | 250 kg | 551 lb (mass) | ASTM D2783 |
ExxonMobil 32 Mobil Mist Lube Series Mobil Mist Lube Series are extra high performance oils designed for the oil-fog or mist-lubrication of machine components such as slideways, bearings, gears, chains etc. They are formulated from hig.. |
|||
Four Ball Extreme Pressure, Weld Load | 250 kg | 551 lb (mass) | ASTM D2783 |
ExxonMobil 3200 Mobilgear SHC Series The Mobilgear SHC Series lubricants are heavy-duty gear oils primarily designed for all kinds of enclosed gearing as well as plain and rolling element bearings. They are formulated from wax-free pol.. |
|||
Four Ball Extreme Pressure, Weld Load | 250 kg | 551 lb (mass) | ASTM D2783 |
ExxonMobil 627 Mobilgear 600 Series The Mobilgear 600 Series are extra high performance gear oils having outstanding extreme pressure characteristics and load-carrying properties, intended for use in all types of enclosed gear drives .. |
|||
Four Ball Extreme Pressure, Weld Load | 250 kg | 551 lb (mass) | ASTM D2783 |
ExxonMobil 632 Mobilgear 600 Series The Mobilgear 600 Series are extra high performance gear oils having outstanding extreme pressure characteristics and load-carrying properties, intended for use in all types of enclosed gear drives .. |
|||
Four Ball Extreme Pressure, Weld Load | 250 kg | 551 lb (mass) | ASTM D2783 |
ExxonMobil Spartan EP 460 Exxon SPARTAN EP lubricants are a family of premium quality extreme pressure gear lubricants. They are formulated with high quality mineral oils, which help reduce sludge formation and oil thickenin.. |
|||
Four Ball Extreme Pressure, Weld Load | 250 kg | 551 lb (mass) | ASTM D2596 |
ExxonMobil 460 Mobilith SHC Series Mobilith SHC Series greases are supreme performance products designed for a wide variety of applications at extremes of temperature. They combine the unique features of synthetic base fluids with th.. |
|||
Four Ball Extreme Pressure, Weld Load | 250 kg | 551 lb (mass) | ASTM D2596 |
ELM® SoyLube® All Purpose Lubricant and Penetrating Oil Description: SoyLube All Purpose Lubricant and Penetrating Oil is a high performance, biodegradable penetrant and lubricating oil for general purpose use. Formulated with the best optimized USA-gro.. |
|||
Four Ball Extreme Pressure, Weld Load | 250 kg | 551 lb (mass) | Load Weld Point; ASTM D2783 |
ChevronTexaco ISO 320 Ultra Gear Lubricant FeaturesChevron Ultra Gear Lubricants are premium grade, multipurpose gear lubricants.They are formulated with a unique extreme pressure additive using an inorganic borate compound. ISO 68, 150, 220.. |
|||
Four Ball Extreme Pressure, Weld Load | 250 kg | 551 lb (mass) | Load Weld Point; ASTM D2783 |
ChevronTexaco ISO 68 Ultra Gear Lubricant FeaturesChevron Ultra Gear Lubricants are premium grade, multipurpose gear lubricants.They are formulated with a unique extreme pressure additive using an inorganic borate compound. ISO 68, 150, 220.. |
|||
Four Ball Extreme Pressure, Weld Load | 250 kg | 551 lb (mass) | Load Weld Point; ASTM D2783 |
ChevronTexaco ISO 680 Ultra Gear Lubricant FeaturesChevron Ultra Gear Lubricants are premium grade, multipurpose gear lubricants.They are formulated with a unique extreme pressure additive using an inorganic borate compound. ISO 68, 150, 220.. |
|||
Four Ball Extreme Pressure, Weld Load | 250 kg | 551 lb (mass) | |
ChevronTexaco Novatex® EP NLGI Grade 000 Texaco Novatex EP are water resistant, extreme pressure greases. They are manufactured using highly refined, select high viscosity index base oils, a calcium soap, and a specifically selected addit.. |
|||
Four Ball Extreme Pressure, Weld Load | 250 kg | 551 lb (mass) | |
ChevronTexaco Novatex® EP NLGI Grade 1 Texaco Novatex EP are water resistant, extreme pressure greases. They are manufactured using highly refined, select high viscosity index base oils, a calcium soap, and a specifically selected addit.. |
|||
Four Ball Extreme Pressure, Weld Load | 250 kg | 551 lb (mass) | |
ChevronTexaco Starplex® HD 6802 NLGI Grade 2 Texaco Starplex HD 6802 delivers value through:Good water resistance — Strong resistance to wash out of bearings.Good rust and corrosion protection, even in wet conditions.Extreme pressure protecti.. |
|||
Four Ball Extreme Pressure, Weld Load | 250 kg | 551 lb (mass) | ASTM D2596 |
ExxonMobil 100 Mobilith SHC Series Mobilith SHC Series greases are supreme performance products designed for a wide variety of applications at extremes of temperature. They combine the unique features of synthetic base fluids with th.. |
|||
Four Ball Extreme Pressure, Weld Load | >= 250 kg | >= 551 lb (mass) | ASTM D2596 |
ExxonMobil 100 Special Mobiltemp SHC Series Mobiltemp SHC Series products are supreme performance antiwear greases primarily intended for high temperature applications. They combine the unique features of polyalphaolefin (PAO) synthetic base .. |
|||
Four Ball Extreme Pressure, Weld Load | 250 kg | 551 lb (mass) | ASTM D2783 |
ExxonMobil 150 Mobilgear SHC Series The Mobilgear SHC Series lubricants are heavy-duty gear oils primarily designed for all kinds of enclosed gearing as well as plain and rolling element bearings. They are formulated from wax-free pol.. |
|||
Four Ball Extreme Pressure, Weld Load | 250 kg | 551 lb (mass) | ASTM D2783 |
ExxonMobil 27 Mobil Mist Lube Series Mobil Mist Lube Series are extra high performance oils designed for the oil-fog or mist-lubrication of machine components such as slideways, bearings, gears, chains etc. They are formulated from hig.. |
|||
Four Ball Extreme Pressure, Weld Load | 250 kg | 551 lb (mass) | ASTM D2783 |
ExxonMobil 626 Mobilgear 600 Series The Mobilgear 600 Series are extra high performance gear oils having outstanding extreme pressure characteristics and load-carrying properties, intended for use in all types of enclosed gear drives .. |
|||
Four Ball Extreme Pressure, Weld Load | 250 kg | 551 lb (mass) | ASTM D2783 |
ExxonMobil 680 Mobilgear SHC Series The Mobilgear SHC Series lubricants are heavy-duty gear oils primarily designed for all kinds of enclosed gearing as well as plain and rolling element bearings. They are formulated from wax-free pol.. |
|||
Four Ball Extreme Pressure, Weld Load | 250 kg | 551 lb (mass) | ASTM D2783 |
ExxonMobil Spartan EP 150 Exxon SPARTAN EP lubricants are a family of premium quality extreme pressure gear lubricants. They are formulated with high quality mineral oils, which help reduce sludge formation and oil thickenin.. |
|||
Four Ball Extreme Pressure, Weld Load | 250 kg | 551 lb (mass) | ASTM D2783 |
ExxonMobil Spartan EP 320 Exxon SPARTAN EP lubricants are a family of premium quality extreme pressure gear lubricants. They are formulated with high quality mineral oils, which help reduce sludge formation and oil thickenin.. |
|||
Four Ball Extreme Pressure, Weld Load | 250 kg | 551 lb (mass) | ASTM D2783 |
ExxonMobil Spartan EP 680 Exxon SPARTAN EP lubricants are a family of premium quality extreme pressure gear lubricants. They are formulated with high quality mineral oils, which help reduce sludge formation and oil thickenin.. |
|||
Four Ball Extreme Pressure, Weld Load | 250 kg | 551 lb (mass) | |
ConocoPhillips EP Conolith® Grease NLGI NO. 2 Description: Conoco EP Conolith Grease is a high-quality, multipurpose, extreme pressure lithium grease recommended for heavy-duty, heavily loaded antifriction and plain bearings. It is ideal for th.. |
|||
Four Ball Extreme Pressure, Weld Load | 250 kg | 551 lb (mass) | |
ConocoPhillips Moly Poly Grease NLGI No. 2 Description: Conoco Moly Poly Grease is a long-life, lithium 12-hydroxy grease for chassis, wheel bearings, ball joints, U-joints, tie-rod ends, steering knuckles and brake self-adjusting screws fou.. |