ExxonMobil Spartan EP 150

Category Fluid , Lubricant
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Spartan EP 150.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Exxon SPARTAN EP lubricants are a family of premium quality extreme pressure gear lubricants. They are formulated with high quality mineral oils, which help reduce sludge formation and oil thickening, therefore increasing oil service life. SPARTAN EP oils contain a sulphur / phosphorus extreme pressure additive system that gives high load carrying ability and protection against wear. In addition these oils provide excellent protection against corrosion of steel and copper containing alloys. SPARTAN EP oils have good water handling properties: water separates from them rapidly preventing contamination of the system, and they are resistant to foam formation. SPARTAN EP oils can be used in either splash or circulating systems. SPARTAN EP gear oils are suitable for use wherever an industrial gear oil is required, and are particularly useful for use at high temperatures, up to 95°C. SPARTAN EP grades are suitable for the lubrication of heavily loaded enclosed gear sets including spur, helical and bevel designs and provide protection in applications where shock loading occurs. SPARTAN EP may also be used in worm gears, though a maximum temperature of 85°C is recommended for continuous operation. They may also be used for lubrication of plain bearings, and in rolling contact (anti-friction) bearings. They also find broad usage in marine gear applications.Exxon SPARTAN EP gear oils are used in a wide range of industrial spur, helical, bevel and steel-on-steel worm gearing as well as marine applications. Specific applications include: Drives for conveyers, agitators, dryers, fans, mixers, presses, pulpers, pumps, screens, extruders, oil well pumps; Industrial bearings journal and rolling contact, especially operating at low speeds and high loads; Drives for main propulsion, centrifuges, deck machinery such as winches, windlasses, cranes, turning gears, pumps, elevators and rudder carriers
Physical Properties Metric English Comments
Density 0.890 g/cc

@Temperature 15.6 °C
0.0322 lb/in³

@Temperature 60.1 °F
ASTM D4052
Viscosity Measurement 98
98
Index; ASTM D2270
Kinematic Viscosity at 40°C (104°F) 150 cSt
150 cSt
ASTM D445
Kinematic Viscosity at 100°C (212°F) 15.8 cSt
15.8 cSt
ASTM D445
Mechanical Properties Metric English Comments
Four Ball Extreme Pressure, Load Wear Index 48
48
ASTM D2783
Four Ball Extreme Pressure, Weld Load 250 kg
551 lb (mass)
ASTM D2783
Timken Test 29500 g
65.0 lb
Thermal Properties Metric English Comments
Pour Point -27.0 °C
-16.6 °F
ASTM D97
Flash Point 245 °C
473 °F
ASTM D92
Descriptive Properties Value Comments
Copper Strip Corrosion 1B
3 hrs @ 100°C
Demulsibility Time (min) 30
to 3 mL emulsion @ 82°C
Foam Sequence II, ASTM D893 0/0
FZG Scuffing, DIN 5182, A/8.3/90, Fail Stage 12+
Rust Prevention, Synthetic Sea Water pass
ASTM D665B