Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 14.0 - 95.0 kJ/m² | 6.66 - 45.2 ft-lb/in² | Average value: 68.0 kJ/m² Grade Count:3 |
Overview of materials for Liquid Crystal Polymer (LCP), Unfilled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), Unfilled". Each property range of values reported is minimum and maximum v.. |
|||
Izod Impact, Notched (ISO) | 2.50 - 95.0 kJ/m² | 1.19 - 45.2 ft-lb/in² | Average value: 13.0 kJ/m² Grade Count:240 |
Overview of materials for Nylon 66, 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. .. |