Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 3.00 - 4.50 kJ/m² | 1.43 - 2.14 ft-lb/in² | Average value: 3.83 kJ/m² Grade Count:3 |
Overview of materials for Phenolic, Novolac, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Glass Filled". Each property range of values reported is minimum and maximum values o.. |
|||
Izod Impact, Notched (ISO) | 4.00 - 4.50 kJ/m² | 1.90 - 2.14 ft-lb/in² | Average value: 4.25 kJ/m² Grade Count:4 |
Overview of materials for Acetal Homopolymer, PTFE-Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, PTFE-Filled". Each property range of values reported is minimum and maximum values o.. |