Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 1.80 - 4.00 kJ/m² @Temperature -40.0 - -20.0 °C |
0.857 - 1.90 ft-lb/in² @Temperature -40.0 - -4.00 °F |
Average value: 2.41 kJ/m² Grade Count:7 |
Overview of materials for Polypropylene with 20% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Talc Filler".Specific grades with primary filler content between 15% and 24% are .. |
|||
Izod Impact, Notched (ISO) | 2.00 - 4.00 kJ/m² @Temperature -30.0 - -30.0 °C |
0.952 - 1.90 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 2.96 kJ/m² Grade Count:5 |
Overview of materials for Styrene-Butadiene Copolymer, SBC This property data is a summary of similar materials in the MatWeb database for the category "Styrene-Butadiene Copolymer, SBC". Each property range of values reported is minimum and maximum values .. |
|||
Izod Impact, Notched (ISO) | 2.00 - 4.00 kJ/m² @Temperature -40.0 - -20.0 °C |
0.952 - 1.90 ft-lb/in² @Temperature -40.0 - -4.00 °F |
Average value: 3.00 kJ/m² Grade Count:4 |
Overview of materials for Nylon 6, 20% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 20% Mineral Filled". Specific grades with primary filler content between 15% and 24% are includ.. |
|||
Izod Impact, Notched (ISO) | 3.00 - 4.00 kJ/m² @Temperature -40.0 - -20.0 °C |
1.43 - 1.90 ft-lb/in² @Temperature -40.0 - -4.00 °F |
Average value: 3.50 kJ/m² Grade Count:1 |
Overview of materials for Nylon 66, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Extruded". Each property range of values reported is minimum and maximum values of appropriate.. |
|||
Izod Impact, Notched (ISO) | 3.00 - 4.00 kJ/m² @Temperature -40.0 - -20.0 °C |
1.43 - 1.90 ft-lb/in² @Temperature -40.0 - -4.00 °F |
Average value: 3.56 kJ/m² Grade Count:3 |
Overview of materials for Nylon 66, 10% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Mineral Filled". Specific grades with primary filler content between 5% and 14% are includ.. |
|||
Izod Impact, Notched (ISO) | 3.00 - 4.00 kJ/m² @Temperature -40.0 - -20.0 °C |
1.43 - 1.90 ft-lb/in² @Temperature -40.0 - -4.00 °F |
Average value: 3.67 kJ/m² Grade Count:1 |
Overview of materials for Nylon 6, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Extruded". Each property range of values reported is minimum and maximum values of appropriate .. |
|||
Izod Impact, Notched (ISO) | 3.00 - 4.00 kJ/m² @Temperature -40.0 - -20.0 °C |
1.43 - 1.90 ft-lb/in² @Temperature -40.0 - -4.00 °F |
Average value: 3.50 kJ/m² Grade Count:2 |
Overview of materials for Nylon 6, Nucleated This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Nucleated". Each property range of values reported is minimum and maximum values of appropriate.. |
|||
Izod Impact, Notched (ISO) | 4.00 - 4.00 kJ/m² @Temperature -30.0 - -30.0 °C |
1.90 - 1.90 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 4.00 kJ/m² Grade Count:1 |
Overview of materials for Polypropylene Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene Glass Bead Filled". Each property range of values reported is minimum and maximum values o.. |
|||
Izod Impact, Notched (ISO) | 2.00 - 4.00 kJ/m² | 0.952 - 1.90 ft-lb/in² | Average value: 3.38 kJ/m² Grade Count:4 |
Overview of materials for Polyphenylene Sulfide (PPS), Unreinforced, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Unreinforced, Extruded". Each property range of values reported is minimum .. |
|||
Izod Impact, Notched (ISO) | 4.00 - 4.00 kJ/m² @Temperature -30.0 - -30.0 °C |
1.90 - 1.90 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 4.00 kJ/m² Grade Count:1 |
Overview of materials for Polyphthalamide (PPA), Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Mineral Filled". Each property range of values reported is minimum and maximum values o.. |