Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 2.40 - 28.0 kJ/m² | 1.14 - 13.3 ft-lb/in² | Average value: 8.43 kJ/m² Grade Count:14 |
Overview of materials for Polypropylene with 20% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Talc Filler".Specific grades with primary filler content between 15% and 24% are .. |
|||
Izod Impact, Notched (ISO) | 2.40 - 16.0 kJ/m² | 1.14 - 7.61 ft-lb/in² | Average value: 5.97 kJ/m² Grade Count:55 |
Overview of materials for Nylon 6, Glass/Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass/Mineral Reinforced". Each property range of values reported is minimum and maximum values.. |
|||
Izod Impact, Notched (ISO) | 2.40 kJ/m² | 1.14 ft-lb/in² | ISO 180/1A |
Lucite International Diakon® TD510 Toughened Acrylic Compound The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness.The grades in the Diakon® series can be processed by.. |
|||
Izod Impact, Notched (ISO) | 2.40 kJ/m² | 1.14 ft-lb/in² | Type 1, Notch A; ISO 180 |
Solvay Specialty Polymers Lavanta® 5115 WH224 Polyester, High Performance (HPP), 15% Glass Fiber Lavanta® 5115 WH224 is a 15% glass fiber reinforced, high-performance polyester (HPP) injection molding grade developed specifically for HB LED packaging applications that utilize surface mount t.. |
|||
Izod Impact, Notched (ISO) | 2.40 kJ/m² | 1.14 ft-lb/in² | ASTM D256 |
Tipco Tipcolite® TG 618 Phenolic Compound, Mineral & Wood Flour, Medium Flow & High Electrical Properties Medium Flow Phenolic Compound, Reinforced with Mineral & Wood FlourApplications: Electrical & ElectronicsProcessing: Compression & TransferInformation provided by the Manufacturer, Tipco Industrie.. |
|||
Izod Impact, Notched (ISO) | 2.40 kJ/m² | 1.14 ft-lb/in² | ISO 180 |
BASF Ultramid® SEGM35 H1 BK 6259 40% Glass/Mineral Filled PA6 (Dry) Description: Ultramid SEGM35 H1 BK6259 is a 40% glass/mineral reinforced injection molding grade. It offers enhanced surface appearance, it also exhibits similar UV weathering characteristics compar.. |
|||
Izod Impact, Notched (ISO) | 2.40 kJ/m² | 1.14 ft-lb/in² | ISO 180/1A |
A.D. Compound Adene NCWA Homopolymer 60% CaCO3 Filled Polypropylene Information provided by A.D. Compound |