Polymer Property : Izod Impact, Notched (ISO) = 7.00 kJ/m² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 7.00 - 7.00 kJ/m²

@Temperature -30.0 - -30.0 °C
3.33 - 3.33 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 7.00 kJ/m² Grade Count:1
Overview of materials for Polybutylene Terephthalate (PBT), Extrusion Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Extrusion Grade". Each property range of values reported is minimum an..
Izod Impact, Notched (ISO) 7.00 - 7.00 kJ/m²

@Temperature -30.0 - -30.0 °C
3.33 - 3.33 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 7.00 kJ/m² Grade Count:1
Overview of materials for Polyphthalamide (PPA), Carbon Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Carbon Fiber". Each property range of values reported is minimum and maximum values of ..
Izod Impact, Notched (ISO) 5.00 - 7.00 kJ/m²

@Temperature -40.0 - -30.0 °C
2.38 - 3.33 ft-lb/in²

@Temperature -40.0 - -22.0 °F
Average value: 5.88 kJ/m² Grade Count:16
Overview of materials for Acetal Copolymer, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Unreinforced". Each property range of values reported is minimum and maximum values of..
Izod Impact, Notched (ISO) 3.00 - 7.00 kJ/m²
1.43 - 3.33 ft-lb/in²
Average value: 5.14 kJ/m² Grade Count:9
Overview of materials for Acetal Copolymer, 20% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% ar..
Izod Impact, Notched (ISO) 5.00 - 7.00 kJ/m²
2.38 - 3.33 ft-lb/in²
Average value: 5.75 kJ/m² Grade Count:4
Overview of materials for Acetal Copolymer, Steel Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Steel Filled". Each property range of values reported is minimum and maximum values of..
Izod Impact, Notched (ISO) 7.00 - 7.00 kJ/m²

@Temperature -30.0 - -30.0 °C
3.33 - 3.33 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 7.00 kJ/m² Grade Count:1
Overview of materials for Acetal Copolymer, Aramid Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Aramid Fiber Filled". Each property range of values reported is minimum and maximum va..
Izod Impact, Notched (ISO) 7.00 - 7.00 kJ/m²

@Temperature -40.0 - -40.0 °C
3.33 - 3.33 ft-lb/in²

@Temperature -40.0 - -40.0 °F
Average value: 13.1 kJ/m² Grade Count:1
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Extruded". Each property range of values reported is minimum and ..
Izod Impact, Notched (ISO) 7.00 - 7.00 kJ/m²

@Thickness 4.00 - 4.00 mm
3.33 - 3.33 ft-lb/in²

@Thickness 0.157 - 0.157 in
Average value: 13.1 kJ/m² Grade Count:1
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Extruded". Each property range of values reported is minimum and ..
Izod Impact, Notched (ISO) 4.00 - 7.00 kJ/m²
1.90 - 3.33 ft-lb/in²
Average value: 5.00 kJ/m² Grade Count:3
Overview of materials for Polyphenylene Sulfide (PPS); Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS); Molded". Each property range of values reported is minimum and maximum valu..
Izod Impact, Notched (ISO) 7.00 - 7.00 kJ/m²

@Temperature -30.0 - -30.0 °C
3.33 - 3.33 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 7.00 kJ/m² Grade Count:1
Overview of materials for Polyphenylene Sulfide (PPS); Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS); Molded". Each property range of values reported is minimum and maximum valu..
Izod Impact, Notched (ISO) 2.00 - 7.00 kJ/m²

@Temperature -40.0 - -20.0 °C
0.952 - 3.33 ft-lb/in²

@Temperature -40.0 - -4.00 °F
Average value: 3.71 kJ/m² Grade Count:5
Overview of materials for Nylon 66, Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Bead Filled". Each property range of values reported is minimum and maximum values of ap..
Izod Impact, Notched (ISO) 6.00 - 7.00 kJ/m²

@Temperature -40.0 - -20.0 °C
2.86 - 3.33 ft-lb/in²

@Temperature -40.0 - -4.00 °F
Average value: 6.50 kJ/m² Grade Count:1
Overview of materials for Nylon 66, 30% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Carbon Fiber Filled". Specific grades with carbon fiber content between 25% and 34% are in..
Izod Impact, Notched (ISO) 0.700 - 7.00 kJ/m²

@Temperature -40.0 - -30.0 °C
0.333 - 3.33 ft-lb/in²

@Temperature -40.0 - -22.0 °F
Average value: 4.58 kJ/m² Grade Count:12
Overview of materials for Nylon 66, 40% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Mineral Filled". Specific grades with primary filler content between 35% and 44% are inclu..
Izod Impact, Notched (ISO) 7.00 - 7.00 kJ/m²

@Temperature -30.0 - -30.0 °C
3.33 - 3.33 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 7.00 kJ/m² Grade Count:1
Overview of materials for Nylon 6, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, PTFE Filled". Each property range of values reported is minimum and maximum values of appropria..
Izod Impact, Notched (ISO) 3.50 - 7.00 kJ/m²
1.67 - 3.33 ft-lb/in²
Average value: 4.79 kJ/m² Grade Count:14
Overview of materials for Acetal Copolymer, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, PTFE Filled". Each property range of values reported is minimum and maximum values of ..
Izod Impact, Notched (ISO) 3.00 - 7.00 kJ/m²
1.43 - 3.33 ft-lb/in²
Average value: 4.65 kJ/m² Grade Count:4
Overview of materials for Polybutylene Terephthalate (PBT), PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), PTFE Filled". Each property range of values reported is minimum and ma..
Izod Impact, Notched (ISO) 7.00 - 7.00 kJ/m²

@Temperature -30.0 - -30.0 °C
3.33 - 3.33 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 7.00 kJ/m² Grade Count:1
Overview of materials for Polysulfone, 20% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are inc..
Izod Impact, Notched (ISO) 7.00 - 7.00 kJ/m²

@Temperature -30.0 - -30.0 °C
3.33 - 3.33 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 7.00 kJ/m² Grade Count:1
Overview of materials for Polysulfone, 30% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are inc..
Izod Impact, Notched (ISO) 4.00 - 7.00 kJ/m²
1.90 - 3.33 ft-lb/in²
Average value: 5.33 kJ/m² Grade Count:3
Overview of materials for Polybutylene Terephthalate (PBT), Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Carbon Fiber Filled". Each property range of values reported is minimu..