Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 6.00 - 40.0 kJ/m² @Temperature -40.0 - -10.0 °C |
2.86 - 19.0 ft-lb/in² @Temperature -40.0 - 14.0 °F |
Average value: 12.9 kJ/m² Grade Count:13 |
Overview of materials for Polybutylene Terephthalate (PBT), Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Impact Grade". Each property range of values reported is minimum and m.. |
|||
Izod Impact, Notched (ISO) | 12.0 - 40.0 kJ/m² | 5.71 - 19.0 ft-lb/in² | Average value: 25.2 kJ/m² Grade Count:34 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded". Each property range of values reported is .. |
|||
Izod Impact, Notched (ISO) | 7.00 - 40.0 kJ/m² @Temperature -30.0 - -30.0 °C |
3.33 - 19.0 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 17.5 kJ/m² Grade Count:7 |
Overview of materials for Polycarbonate, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Impact Modified". Each property range of values reported is minimum and maximum values of.. |
|||
Izod Impact, Notched (ISO) | 2.70 - 40.0 kJ/m² | 1.28 - 19.0 ft-lb/in² | Average value: 13.1 kJ/m² Grade Count:5 |
Overview of materials for Polypropylene with 30% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Talc Filler". Specific grades with primary filler content between 25% and 34% are.. |