Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 7.30 - 30.0 kJ/m² | 3.47 - 14.3 ft-lb/in² | Average value: 13.3 kJ/m² Grade Count:9 |
Overview of materials for Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled". Specific grades with glass content between 45.. |
|||
Izod Impact, Notched (ISO) | 7.30 kJ/m² | 3.47 ft-lb/in² | ISO 180 |
LNP Thermocomp® GF-1006 Polysulfone, Glass Fiber Reinforcement
(discontinued **) Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names.. |
|||
Izod Impact, Notched (ISO) | 7.30 kJ/m² | 3.47 ft-lb/in² | ISO 180-1A |
Gromax BFG30-DN00N1 Nylon 6 30% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Izod Impact, Notched (ISO) | 7.30 kJ/m² | 3.47 ft-lb/in² | ISO 180/1A |
Cathay PA510 Renewable Engineering Polyamide Cathay engineering polyamides contain 26-100% renewably sourced material. Advantages: Operates at similar conditions to PA66; Suitable for injection, compounding and extrusion; Stable mechanical pr.. |
|||
Izod Impact, Notched (ISO) | 7.30 kJ/m² | 3.47 ft-lb/in² | ISO 180 |
BASF Ultramid® 66 H2 G/25-V0KB1 BK 3324 PA66 (Dry) Description: Ultramid 66 H2 G/25-V0KB1 BK3324 is a 25% glass reinforced, heat stabilized injection molding grade. It's a V-0 self-extinguishing, with phosphorous. It offers good flowability, surface.. |