Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 11.6 kJ/m² | 5.52 ft-lb/in² | ISO 180 |
LNP Thermocomp® LF-1006 Polyetheretherketone, Glass Fiber Reinforcement
(discontinued **) Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names.. |
|||
Izod Impact, Notched (ISO) | 11.6 kJ/m² | 5.52 ft-lb/in² | ISO Test |
BASF Ultramid® SEG8 BK-126 40% Glass Filled PA6 (Dry) Ultramid SEG8 BK-126 is a 40% glass reinforced, pigmented black, injection molding type 6 nylon requiring high strength, surface aesthetics, and good processability. This product has excellent surf.. |