Polymer Property : Izod Impact, Unnotched (ISO) = 9.52 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched (ISO) 20.0 - 20.0 kJ/m²

@Temperature -30.0 - -30.0 °C
9.52 - 9.52 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 20.0 kJ/m² Grade Count:1
Overview of materials for Polystyrene, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Impact Modified". Each property range of values reported is minimum and maximum values of a..
Izod Impact, Unnotched (ISO) 20.0 - 20.0 kJ/m²

@Temperature -30.0 - -30.0 °C
9.52 - 9.52 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 20.0 kJ/m² Grade Count:1
Overview of materials for Polystyrene + Polyphenylene Ether, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene + Polyphenylene Ether, Unreinforced". Each property range of values reported is minimum and ..
Izod Impact, Unnotched (ISO) 18.0 - 20.0 kJ/m²
8.57 - 9.52 ft-lb/in²
Average value: 19.3 kJ/m² Grade Count:3
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled". Specific grades with glass content betwe..
Izod Impact, Unnotched (ISO) 15.0 - 20.0 kJ/m²
7.14 - 9.52 ft-lb/in²
Average value: 17.7 kJ/m² Grade Count:3
Overview of materials for Polypropylene with 20% Calcium Carbonate (CaCO3) Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Calcium Carbonate (CaCO3) Filler". Each property range of values reported is mini..
Izod Impact, Unnotched (ISO) 20.0 - 20.0 kJ/m²

@Temperature -30.0 - -30.0 °C
9.52 - 9.52 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 20.0 kJ/m² Grade Count:2
Overview of materials for Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled". Specific grades with glass content between 35% an..
Izod Impact, Unnotched (ISO) 8.00 - 20.0 kJ/m²
3.81 - 9.52 ft-lb/in²
Average value: 16.0 kJ/m² Grade Count:3
Overview of materials for High Density Polyethylene (HDPE), Injection Molded
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Injection Molded". Each property range of values reported is minimum a..
Izod Impact, Unnotched (ISO) 10.0 - 20.0 kJ/m²
4.76 - 9.52 ft-lb/in²
Average value: 16.0 kJ/m² Grade Count:3
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Stainless Steel Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Stainless Steel Fiber Filled". Each property range of values repo..
Copyright © lookpolymers.com All Rights Reserved