Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 30.0 - 80.0 kJ/m² | 14.3 - 38.1 ft-lb/in² | Average value: 52.4 kJ/m² Grade Count:45 |
Overview of materials for Polybutylene Terephthalate (PBT), Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Flame Retardant". Each property range of values reported is minimum an.. |
|||
Izod Impact, Unnotched (ISO) | 33.0 - 80.0 kJ/m² | 15.7 - 38.1 ft-lb/in² | Average value: 52.0 kJ/m² Grade Count:3 |
Overview of materials for Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled". Specific grades with glass content between 45.. |
|||
Izod Impact, Unnotched (ISO) | 27.0 - 80.0 kJ/m² @Temperature -30.0 - -30.0 °C |
12.8 - 38.1 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 46.8 kJ/m² Grade Count:5 |
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled". Each property range of values repor.. |
|||
Izod Impact, Unnotched (ISO) | 15.0 - 80.0 kJ/m² | 7.14 - 38.1 ft-lb/in² | Average value: 34.0 kJ/m² Grade Count:18 |
Overview of materials for Nylon 6, Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Bead Filled". Each property range of values reported is minimum and maximum values of app.. |
|||
Izod Impact, Unnotched (ISO) | 76.0 - 80.0 kJ/m² @Temperature -30.0 - -30.0 °C |
36.2 - 38.1 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 78.0 kJ/m² Grade Count:2 |
Overview of materials for Nylon 66/6, 60% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 60% Glass Fiber Reinforced". Specific grades with glass content between 55% and 64% are incl.. |
|||
Izod Impact, Unnotched (ISO) | 10.0 - 80.0 kJ/m² | 4.76 - 38.1 ft-lb/in² | Average value: 34.7 kJ/m² Grade Count:9 |
Overview of materials for Nylon 66, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, PTFE Filled". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Izod Impact, Unnotched (ISO) | 11.0 - 80.0 kJ/m² | 5.23 - 38.1 ft-lb/in² | Average value: 31.5 kJ/m² Grade Count:9 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Bead Filled". Each property range of values reported is minimum .. |