Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 33.0 - 50.0 kJ/m² @Temperature -30.0 - -30.0 °C |
15.7 - 23.8 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 44.3 kJ/m² Grade Count:3 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant". Each property range of values re.. |
|||
Izod Impact, Unnotched (ISO) | 36.0 - 50.0 kJ/m² @Temperature -25.0 - 120 °C |
17.1 - 23.8 ft-lb/in² @Temperature -13.0 - 248 °F |
Average value: 41.3 kJ/m² Grade Count:1 |
Overview of materials for Polysulfone (PSU) This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone". Each property range of values reported is minimum and maximum values of appropriate MatWeb.. |
|||
Izod Impact, Unnotched (ISO) | 30.0 - 50.0 kJ/m² | 14.3 - 23.8 ft-lb/in² | Average value: 43.1 kJ/m² Grade Count:9 |
Overview of materials for PBT + ASA Blend, Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "PBT + ASA Blend, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum .. |
|||
Izod Impact, Unnotched (ISO) | 25.0 - 50.0 kJ/m² @Temperature -30.0 - -30.0 °C |
11.9 - 23.8 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 41.0 kJ/m² Grade Count:8 |
Overview of materials for PBT + ASA Blend, Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "PBT + ASA Blend, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum .. |
|||
Izod Impact, Unnotched (ISO) | 45.0 - 50.0 kJ/m² @Temperature -30.0 - -30.0 °C |
21.4 - 23.8 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 47.5 kJ/m² Grade Count:2 |
Overview of materials for Nylon 6, Glass/Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass/Mineral Reinforced". Each property range of values reported is minimum and maximum values.. |
|||
Izod Impact, Unnotched (ISO) | 18.0 - 50.0 kJ/m² @Temperature -30.0 - -30.0 °C |
8.57 - 23.8 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 31.0 kJ/m² Grade Count:3 |
Overview of materials for Nylon 66, Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Bead Filled". Each property range of values reported is minimum and maximum values of ap.. |
|||
Izod Impact, Unnotched (ISO) | 40.0 - 50.0 kJ/m² @Temperature -30.0 - -30.0 °C |
19.0 - 23.8 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 45.0 kJ/m² Grade Count:1 |
Overview of materials for Nylon 66, Glass/Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass/Mineral Filled". Each property range of values reported is minimum and maximum values of.. |
|||
Izod Impact, Unnotched (ISO) | 36.0 - 50.0 kJ/m² @Temperature -25.0 - 120 °C |
17.1 - 23.8 ft-lb/in² @Temperature -13.0 - 248 °F |
Average value: 41.3 kJ/m² Grade Count:1 |
Overview of materials for Polysulfone, 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are inc.. |