Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 46.0 - 48.0 kJ/m² | 21.9 - 22.8 ft-lb/in² | Average value: 46.7 kJ/m² Grade Count:3 |
Overview of materials for Thermoplastic Olefinic Elastomer (TPO) This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Olefinic Elastomer (TPO)". Each property range of values reported is minimum and maximum v.. |
|||
Izod Impact, Unnotched (ISO) | 40.0 - 48.0 kJ/m² | 19.0 - 22.8 ft-lb/in² | Type 1; ISO 180 |
Solvay Specialty Polymers Amodel® HFFR-4133 Polyphthalamide (PPA), 33% Glass Fiber Amodel® HFFR-4133 is a 33% glass-reinforced, halogen-free, flame retardant polyphthalamide (PPA) resin which offers enhanced processing capabilities for electrical and electronic applications. Th.. |
|||
Izod Impact, Unnotched (ISO) | 20.0 - 48.0 kJ/m² | 9.52 - 22.8 ft-lb/in² | Average value: 34.1 kJ/m² Grade Count:24 |
Overview of materials for Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS)- 40% Glass filled; Molded". Specific grades with glass content between 35% a.. |
|||
Izod Impact, Unnotched (ISO) | 40.0 - 48.0 kJ/m² | 19.0 - 22.8 ft-lb/in² | Higher values are for NT and BK324.; ISO 180/1U |
Solvay Specialty Polymers Amodel® HFFR-4133 Polyphthalamide (PPA)
(Unverified Data**) Amodel HFFR-4133 is a 33% glass-reinforced, halogen- free, flame retardant polyphthalamide (PPA) resin which offers enhanced processing capabilities for electrical and electronic applications. This .. |