Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 196 kJ/m² | 93.3 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics EXTEM VH1003M PEI Copolymer Transparent, Thermoplastic Polyimide (TPI) resin with a glass transition temperature (Tg) of 247C. Internal mold release. This product has thinwall FR capability and has a UL94 V0 listing. This mate.. |
|||
Izod Impact, Unnotched (ISO) | 196 kJ/m² | 93.3 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics EXTEM VH1003M PEI Copolymer (Asia Pacific) Transparent, Thermoplastic Polyimide (TPI) resin with a glass transition temperature (Tg) of 247C. Internal mold release. This product has thinwall FR capability and has a UL94 V0 listing. This mate.. |
|||
Izod Impact, Unnotched (ISO) | 196 kJ/m² | 93.3 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics EXTEM VH1003M PEI Copolymer (Europe-Africa-Middle East) Transparent, Thermoplastic Polyimide (TPI) resin. Glass transition Temp. (Tg) of 247°C. Internal mold release. This resin has thinwall FR capability and has a UL94 V0 listing. Resin is halogen free.. |
|||
Izod Impact, Unnotched (ISO) | 196 kJ/m² | 93.3 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics ULTEM XH6050M PEI Copolymer Enhanced flow Polyetherimidesulfone copolymer (Tg 247C) with internal mold release. ECO Conforming, UL94 V0 listing. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774). |
|||
Izod Impact, Unnotched (ISO) | 196 kJ/m² | 93.3 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP STAT-KON RX08408 PA 66 LNP* STAT-KON* RX08404 is a compound based on Nylon 66 containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact. |
|||
Izod Impact, Unnotched (ISO) | 196 kJ/m² @Temperature 23.0 °C |
93.3 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Stat-kon RX08408_NA1D004 PA 66 LNP* Stat-Kon* RX08404_NA1D004 is a compound based on Nylon 66 containing Carbon Powder. Characteristics of this grade include: Electrically Conductive, High Impact.This data was supplied by SABI.. |
|||
Izod Impact, Unnotched (ISO) | 196 kJ/m² | 93.3 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics ULTEM XH6050M PEI Copolymer (Asia Pacific) Enhanced flow Polyetherimidesulfone copolymer (Tg 247C) with internal mold release. ECO Conforming, UL94 V0 listing. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774). |