Polymer Property : Izod Impact, Unnotched (ISO) = 59.5 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched (ISO) 125 kJ/m²
59.5 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP COLORCOMP W10009I PBT (Europe-Africa-Middle East)
LNP* THERMOCOMP* W10009I is a compound based on Polybutylene Terephalate resin containing Flame Retardant.
Izod Impact, Unnotched (ISO) 125 kJ/m²
59.5 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP PI001 PA 6 (Europe-Africa-Middle East)
LNP* LUBRICOMP* PI001 is a compound based on PA 6 resin containing Silicone. Added features include Internally Lubricated.
Izod Impact, Unnotched (ISO) 125 kJ/m²
59.5 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP STAT-KON DX91077 PC
LNP* STAT-KON* DX91077 is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this grade include: Electrically Conductive, Impact Modified.
Izod Impact, Unnotched (ISO) 125 kJ/m²
59.5 ft-lb/in²
ISO 180/1C
Chi Mei Polylac® PA-777D ABS - High Heat
Super High Heat