Mechanical Properties Metric English Comments
Izod Impact, Unnotched (ISO) 35.0 - 70.0 kJ/m²
16.7 - 33.3 ft-lb/in²
Average value: 54.0 kJ/m² Grade Count:39
Overview of materials for Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled". Specific grades with glass content between 25..
Izod Impact, Unnotched (ISO) 41.0 - 70.0 kJ/m²
19.5 - 33.3 ft-lb/in²
Average value: 61.0 kJ/m² Grade Count:4
Overview of materials for Polyaryletherketone (PAEK), Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyaryletherketone (PAEK), Glass Fiber Filled". Each property range of values reported is minimum and m..
Izod Impact, Unnotched (ISO) 15.0 - 70.0 kJ/m²
7.14 - 33.3 ft-lb/in²
Average value: 35.2 kJ/m² Grade Count:26
Overview of materials for Polycarbonate/ABS Alloy, Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Glass Fiber Filled". Each property range of values reported is minimum and maxi..
Izod Impact, Unnotched (ISO) 70.0 - 70.0 kJ/m²

@Temperature -30.0 - -30.0 °C
33.3 - 33.3 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 70.0 kJ/m² Grade Count:1
Overview of materials for Nylon 66, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, PTFE Filled". Each property range of values reported is minimum and maximum values of appropri..
Izod Impact, Unnotched (ISO) 60.0 - 70.0 kJ/m²

@Temperature -30.0 - -30.0 °C
28.6 - 33.3 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 68.0 kJ/m² Grade Count:5
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Molded". Each property range of values reported is minimum and ma..
Izod Impact, Unnotched (ISO) 32.0 - 70.0 kJ/m²
15.2 - 33.3 ft-lb/in²
Average value: 47.3 kJ/m² Grade Count:3
Overview of materials for Polybutylene Terephthalate (PBT), Glass + Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass + Mineral Filled". Each property range of values reported is min..
Izod Impact, Unnotched (ISO) 20.0 - 70.0 kJ/m²
9.52 - 33.3 ft-lb/in²
Average value: 44.8 kJ/m² Grade Count:8
Overview of materials for Nylon 6, 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. ..
Copyright © lookpolymers.com All Rights Reserved