Mechanical Properties Metric English Comments
Izod Impact, Unnotched (ISO) 33.0 - 50.0 kJ/m²

@Temperature -30.0 - -30.0 °C
15.7 - 23.8 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 44.3 kJ/m² Grade Count:3
Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant". Each property range of values re..
Izod Impact, Unnotched (ISO) 36.0 - 50.0 kJ/m²

@Temperature -25.0 - 120 °C
17.1 - 23.8 ft-lb/in²

@Temperature -13.0 - 248 °F
Average value: 41.3 kJ/m² Grade Count:1
Overview of materials for Polysulfone (PSU)
This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone". Each property range of values reported is minimum and maximum values of appropriate MatWeb..
Izod Impact, Unnotched (ISO) 30.0 - 50.0 kJ/m²
14.3 - 23.8 ft-lb/in²
Average value: 43.1 kJ/m² Grade Count:9
Overview of materials for PBT + ASA Blend, Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "PBT + ASA Blend, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum ..
Izod Impact, Unnotched (ISO) 25.0 - 50.0 kJ/m²

@Temperature -30.0 - -30.0 °C
11.9 - 23.8 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 41.0 kJ/m² Grade Count:8
Overview of materials for PBT + ASA Blend, Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "PBT + ASA Blend, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum ..
Izod Impact, Unnotched (ISO) 45.0 - 50.0 kJ/m²

@Temperature -30.0 - -30.0 °C
21.4 - 23.8 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 47.5 kJ/m² Grade Count:2
Overview of materials for Nylon 6, Glass/Mineral Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass/Mineral Reinforced". Each property range of values reported is minimum and maximum values..
Izod Impact, Unnotched (ISO) 18.0 - 50.0 kJ/m²

@Temperature -30.0 - -30.0 °C
8.57 - 23.8 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 31.0 kJ/m² Grade Count:3
Overview of materials for Nylon 66, Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Bead Filled". Each property range of values reported is minimum and maximum values of ap..
Izod Impact, Unnotched (ISO) 40.0 - 50.0 kJ/m²

@Temperature -30.0 - -30.0 °C
19.0 - 23.8 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 45.0 kJ/m² Grade Count:1
Overview of materials for Nylon 66, Glass/Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass/Mineral Filled". Each property range of values reported is minimum and maximum values of..
Izod Impact, Unnotched (ISO) 36.0 - 50.0 kJ/m²

@Temperature -25.0 - 120 °C
17.1 - 23.8 ft-lb/in²

@Temperature -13.0 - 248 °F
Average value: 41.3 kJ/m² Grade Count:1
Overview of materials for Polysulfone, 30% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are inc..
Copyright © lookpolymers.com All Rights Reserved