Polymer Property : Izod Impact, Unnotched (ISO) = 48.0 kJ/m² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched (ISO) 46.0 - 48.0 kJ/m²
21.9 - 22.8 ft-lb/in²
Average value: 46.7 kJ/m² Grade Count:3
Overview of materials for Thermoplastic Olefinic Elastomer (TPO)
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Olefinic Elastomer (TPO)". Each property range of values reported is minimum and maximum v..
Izod Impact, Unnotched (ISO) 40.0 - 48.0 kJ/m²
19.0 - 22.8 ft-lb/in²
Type 1; ISO 180
Solvay Specialty Polymers Amodel® HFFR-4133 Polyphthalamide (PPA), 33% Glass Fiber
Amodel® HFFR-4133 is a 33% glass-reinforced, halogen-free, flame retardant polyphthalamide (PPA) resin which offers enhanced processing capabilities for electrical and electronic applications. Th..
Izod Impact, Unnotched (ISO) 20.0 - 48.0 kJ/m²
9.52 - 22.8 ft-lb/in²
Average value: 34.1 kJ/m² Grade Count:24
Overview of materials for Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS)- 40% Glass filled; Molded". Specific grades with glass content between 35% a..
Izod Impact, Unnotched (ISO) 40.0 - 48.0 kJ/m²
19.0 - 22.8 ft-lb/in²
Higher values are for NT and BK324.; ISO 180/1U
Solvay Specialty Polymers Amodel® HFFR-4133 Polyphthalamide (PPA)  (Unverified Data**)
Amodel HFFR-4133 is a 33% glass-reinforced, halogen- free, flame retardant polyphthalamide (PPA) resin which offers enhanced processing capabilities for electrical and electronic applications. This ..