Polymer Property : Izod Impact, Unnotched (ISO) = 110 kJ/m² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched (ISO) 110 kJ/m²

@Temperature -30.0 °C
52.3 ft-lb/in²

@Temperature -22.0 °F
80*10*3; ISO 180/1U
SABIC Innovative Plastics Lexan® 2814R PC (Europe-Africa-Middle East)
LEXAN 2814R is a high viscosity, 10% glass reinforced, flame retardant grade, especially developed to meet the CSTB M2 flammability rating.
Izod Impact, Unnotched (ISO) 110 kJ/m²

@Temperature 23.0 °C
52.3 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP Faradex MS003XXC PP (Europe-Africa-Middle East)
LNP* Faradex* MS003XXC is a compound based on Polypropylene resin containing Stainless Steel Fiber. Added features of this material include: EMI/RFI Shielding.This data was supplied by SABIC-IP for..
Izod Impact, Unnotched (ISO) 110 kJ/m²
52.3 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP FARADEX MX10014 PP (Europe-Africa-Middle East)
LNP* Faradex* Mx10014 is a compound based on Polypropylene resin containing Stainless Steel Fiber. Added features of this material include: EMI/RFI Shielding.
Izod Impact, Unnotched (ISO) 110 kJ/m²

@Temperature -30.0 °C
52.3 ft-lb/in²

@Temperature -22.0 °F
80*10*3; ISO 180/1U
SABIC Innovative Plastics Lexan® HF500R PC (Europe-Africa-Middle East)
LEXAN HF500R is an easy flow, 9% glass reinforced, flame retardant grade, especially designed for applications requiring high rigidity together with high heat resistance and impact performance.
Izod Impact, Unnotched (ISO) 110 kJ/m²

@Temperature 23.0 °C
52.3 ft-lb/in²

@Temperature 73.4 °F
ISO 180-1U
Lanxess Pocan® DP 7318 000000 PBT, 17% Pigment
PBT, 17% white pigments, injection molding, improved light reflection, low tendency to warpInformation provided by LANXESS.
Izod Impact, Unnotched (ISO) 110 kJ/m²
52.3 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP DL003EXJ PC
LNP* Lubricomp* DL003EXJ is a compound based on Polycarbonate containing 15% PTFE. Characteristics of this grade are Easy Molding, Low Extractable, Internally Lubricated, Healthcare.
Izod Impact, Unnotched (ISO) 110 kJ/m²

@Temperature 23.0 °C
52.3 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP Lubricomp DP003XXP PC (Europe-Africa-Middle East)
LNP* LUBRICOMP* DP003XXP is a compound based on Polycarbonate resin containing PTFE, Silicone. Added features include: Internally Lubricated.This data was supplied by SABIC-IP for the Europe-Africa..
Izod Impact, Unnotched (ISO) 110 kJ/m²
52.3 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics Xenoy® X2420 PC+POLYESTER (Asia Pacific)
Xenoy*X2420 is a 10% glass filled, high flow, impact modified, injection moldable grade designed for high flow and impact strength. X2420 has enhanced melt flowability, impact ductility and broad co..
Izod Impact, Unnotched (ISO) 110 kJ/m²
52.3 ft-lb/in²
DAM; ISO 180/1U
DuPont Performance Polymers Minlon® 12TA BKB124 Nylon 66  (Unverified Data**)
32% Mineral Reinforced Toughened Polyamide 66 Minlon 12TA BKB124 is a 32% mineral reinforced toughened heat stabilized black polyamide 66 resin for injection molding.Information provided by DuPont P..
Izod Impact, Unnotched (ISO) 110 kJ/m²
52.3 ft-lb/in²
80x10x4; ISO 180/1U
Eurostar Star L POM D36 POM, Injection Molded
Star L POM D36 is Molybdenum Disulfide Lubricated, POM Copolymer Injection Molding ResinInformation provided by Eurostar.
Izod Impact, Unnotched (ISO) 110 kJ/m²
52.3 ft-lb/in²
80x10x4; ISO 180/1U
Eurostar Star L POM D74 POM, Injection Molded
Star L POM D74 is a Proprietary Additive Lubricated, POM Copolymer Injection Molding ResinInformation provided by Eurostar.