Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | 17.2 MPa @Temperature -55.0 °C |
2490 psi @Temperature -67.0 °F |
Lap Shear |
Henkel Hysol PL 737 Film Adhesive Nonmetallic, modified epoxy film specifically designed for use in structural aircraft components. Low flow characteristics.Application: Metal and Honeycomb Bonding |
|||
Adhesive Bond Strength | 17.2 MPa @Temperature 23.9 °C |
2490 psi @Temperature 75.0 °F |
on steel; ASTM D1002-64 |
3M Pronto™ CA-7 Instant Adhesive One-part, room-temperature curing adhesive that is ready-to-use without metering or mixing. Bonded parts reach handling strength in 5-10 seconds on many applications.Very fast setting product with .. |
|||
Adhesive Bond Strength | 17.2 MPa @Temperature 132 °C |
2490 psi @Temperature 270 °F |
Lap Shear |
Henkel Hysol PL 795 Film Adhesive Epoxy film adhesive designed for composite bonding applications. May cure at 250°F / 121°C or 350°F / 177°C, with service temperatures up to 350°F / 177°C. Ideal for co-cure or secondary bondi.. |
|||
Adhesive Bond Strength | 17.2 MPa @Temperature -55.0 °C |
2490 psi @Temperature -67.0 °F |
Tensile Lap Shear |
Henkel Hysol EA 9396/C-2 Paste Adhesive System Two-part, elevated cure, unfilled, low viscosity adhesive with structural properties to 400°F / 204°C.Applications: Structural Repair Low Viscosity Wet Lay-Up Composite Bonding |