Polymer Property : Charpy Impact Unnotched = 43.3 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact Unnotched 9.10 J/cm²

@Temperature -30.0 °C
43.3 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Ascend Performance Materials Vydyne® R550 Nylon 66, 50% Glass Reinforced, DAM
Vydyne® R550 is general-purpose, hydrolysis-resistant, 50% glass-fiber reinforced PA66 resin. Available in natural, it is also lubricated for improved flow and offers superior surface appearance. G..
Charpy Impact Unnotched 9.10 J/cm²

@Temperature -30.0 °C
43.3 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Ascend Performance Materials Vydyne® R550H Nylon 66, 50% Glass Reinforced, DAM
Vydyne® R550H is general-purpose, heat-stabilized, hydrolysis-resistant, 50% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of physic..
Charpy Impact Unnotched 9.10 J/cm²

@Temperature -30.0 °C
43.3 ft-lb/in²

@Temperature -22.0 °F
ISO 179
Ascend Performance Materials Vydyne® R633 Nylon 66 Copolymer, 33% Glass Filled, Conditioned (2.5% Moisture)
Vydyne® R633 is 33% glass-fiber reinforced, PA66/6 copolymer resin for superior surface appearance. Available in natural, this injection-molding grade resin is lubricated for machine feed and mold ..
Charpy Impact Unnotched 9.10 J/cm²

@Temperature -30.0 °C
43.3 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Ascend Performance Materials Vydyne® R633H Nylon 66/6, 33% Glass Reinforced, Conditioned
Vydyne® R633H is 33% glass-fiber reinforced PA66/6 copolymer resin for superior surface appearance. Available in natural, this injection-molding grade resin is lubricated for machine feed and mold ..