Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 2.30 J/cm² @Temperature -20.0 °C |
10.9 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVALEN PH 72 T 40 PP, 40% mineral filling FeaturesModified homopolymer PP for injection moulding with the content of 40% microground, floated, thermo stable, chemically modified talc. General application in all industry branches - covers of.. |
|||
Charpy Impact Unnotched | 2.30 J/cm² @Temperature -20.0 °C |
10.9 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVALEN PH 78 T 40 PP, 40% mineral filling FeaturesModified homopolymer PP for injection moulding with the content of 40% microground, floated, chemically modified talc. Stable towards detergents. General application in all industry branches.. |
|||
Charpy Impact Unnotched | 2.30 J/cm² @Temperature -20.0 °C |
10.9 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVALEN PH 92 T 40 PP, 40% mineral filling FeaturesModified homopolymer PP for injection moulding with the content of 40% microground, floated, chemically modified talc. Stable towards oxidants. General application in all industry branches -.. |
|||
Charpy Impact Unnotched | 2.30 J/cm² @Temperature -20.0 °C |
10.9 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVASTER® B GF 6 FRL 4 PBT, 6% glass fibre, flame retarder FeaturesPBT with the content of 6 % chemically bound glass fibre and with the flame retardant on the basis of bromine hydrocarbons. Anisotropy of shrinkage enables the injection moulding of round, c.. |
|||
Charpy Impact Unnotched | 2.30 J/cm² @Temperature 23.0 °C |
10.9 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Polykemi AB POLYfill PPC GF2007 PD1 Polypropylene Copolymer, Glass Fiber Reinforced, Chemically Coupled Information provided by Polykemi AB |
|||
Charpy Impact Unnotched | 2.30 J/cm² @Temperature 23.0 °C |
10.9 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Polykemi AB POLYfill PPH GK8020D Polypropylene Homopolymer, Glass Reinforced, Detergent Resistant Information provided by Polykemi AB |
|||
Charpy Impact Unnotched | 2.30 J/cm² @Temperature 23.0 °C |
10.9 ft-lb/in² @Temperature 73.4 °F |
Conditioned; ISO 179/1eU |
Lanxess Durethan® DP BM 65 X FM30 901510 Nylon 6, 65% Mineral + Glass Fiber PA, injection molding and hybrid grade based on PA 6, 65% mineral/glass fibers, UL 94V-0 at 1.2 mm, reduced cycle times (easy flow), Thin wall application, free from halogen and phosphorous, low smo.. |
|||
Charpy Impact Unnotched | 2.30 J/cm² @Temperature -30.0 °C |
10.9 ft-lb/in² @Temperature -22.0 °F |
|
Radici Radiflam® S RV250FR (dry) Nylon 6 Radiflam® S is a range of flame retardant polyamides 6 (PA 6) used for injection molding and extrusion for all applications where high fire resistance is required.Information provided by Radici gro.. |
|||
Charpy Impact Unnotched | 2.30 J/cm² @Temperature -30.0 °C |
10.9 ft-lb/in² @Temperature -22.0 °F |
|
Radici Radiflam® B RV250AE Polybutylene Terephthalate - 25% Glass fiber reinforced Radiflam® B is a range of flame retardant polybutylene terephthalate (PBT) used for injection molding and extrusion for all applications where high fire resistance is required.Information provided .. |