Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 2.10 J/cm² @Temperature -20.0 °C |
9.99 ft-lb/in² @Temperature -4.00 °F |
STN EN ISO 179 |
Plastcom SLOVALEN PC 51 C 30 Polypropylene Homopolymer and Copolymer, 30% Micronized Talc FeaturesModified homopolymer and copolymer PP for injection moulding with the content of 30% micronized, chemically modified talc. Increased strength, rigidity and thermal application up to 120°C... |
|||
Charpy Impact Unnotched | 2.10 J/cm² @Temperature -20.0 °C |
9.99 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Polykemi AB POLYfill PP CQX30030 RTX Polypropylene, Mineral Reinforced, Scratch Resistant Information provided by Polykemi AB |
|||
Charpy Impact Unnotched | 2.10 J/cm² @Temperature -20.0 °C |
9.99 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Polykemi AB POLYfill PPC GF2007 PD1 Polypropylene Copolymer, Glass Fiber Reinforced, Chemically Coupled Information provided by Polykemi AB |
|||
Charpy Impact Unnotched | 2.10 J/cm² @Temperature -20.0 °C |
9.99 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Polykemi AB POLYfill PPC T12020 Polypropylene Copolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Charpy Impact Unnotched | 2.10 J/cm² @Temperature -20.0 °C |
9.99 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Polykemi AB POLYfill PPC T16020 Polypropylene Copolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Charpy Impact Unnotched | 2.10 J/cm² @Temperature -20.0 °C |
9.99 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Polykemi AB POLYfill PPC T8020 FC Polypropylene Copolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Charpy Impact Unnotched | 2.10 J/cm² @Temperature 23.0 °C |
9.99 ft-lb/in² @Temperature 73.4 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics Ultem 2412EPR PEI 40% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.This data was supplied by SABIC-IP for the Am.. |
|||
Charpy Impact Unnotched | 2.10 J/cm² @Temperature 23.0 °C |
9.99 ft-lb/in² @Temperature 73.4 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics Ultem 2412EPR PEI (Asia Pacific) 40% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.This data was supplied by SABIC-IP for the As.. |
|||
Charpy Impact Unnotched | 2.10 J/cm² @Temperature 23.0 °C |
9.99 ft-lb/in² @Temperature 73.4 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics Ultem 2412EPR PEI (Europe-Africa-Middle East) 40% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.This data was supplied by SABIC-IP for the Eu.. |
|||
Charpy Impact Unnotched | 2.10 J/cm² @Temperature -30.0 °C |
9.99 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Styrolution Luran® HH-120 Alpha-Methylstyrene Acrylonitrile Luran HH-120 is a grade of AMSAN with high heat resistance and improved mechanical strength. It is suitable for injection molding and extrusion applications and can be used as a modifier for high he.. |
|||
Charpy Impact Unnotched | 2.10 J/cm² @Temperature 0.000 °C |
10.0 ft-lb/in² @Temperature 32.0 °F |
ISO 179/1eU |
ExxonMobil Exxtral™ LNU 011 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin with high stiffness, high gloss, low discoloration and good detergent resistance for large electrical appliances such as washing machi.. |