Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 1.10 J/cm² @Temperature -20.0 °C |
5.23 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVAMID 66 T 36 TS PA66, 36% mineral filling FeaturesPA 66 with the content of 36 % chemically modified mineral filling. Used for holders of electric hand tools, for hobby tools, gears, covers of electric tools, flat products, automobile wheel.. |
|||
Charpy Impact Unnotched | 1.10 J/cm² @Temperature -20.0 °C |
5.23 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Polykemi AB POLYfill PPH GK8020D Polypropylene Homopolymer, Glass Reinforced, Detergent Resistant Information provided by Polykemi AB |
|||
Charpy Impact Unnotched | 1.10 - 1.30 J/cm² @Temperature 23.0 °C |
5.24 - 6.19 ft-lb/in² @Temperature 73.4 °F |
Injection; ISO 179/ 1eU |
Raschig Group AMPLA® 7250 melamine-modified polyester Cellulose reinforced melamine-modified Polyester molding compound. Very good electrical values, excellent heat resistance, excellent surface quality, low post shrinkage. This product meets the allow.. |
|||
Charpy Impact Unnotched | 1.10 J/cm² @Temperature -20.0 °C |
5.23 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVALEN PH 92 T 30 PP, 30% mineral filling FeaturesModified PP for injection moulding with the content of 30% mineral filling. Increased rigidity, strength and thermal. Decreased shrinkage. General application in all industry branches.Packag.. |
|||
Charpy Impact Unnotched | 1.10 J/cm² @Temperature -20.0 °C |
5.24 ft-lb/in² @Temperature -4.00 °F |
DIN 53453 |
LATI LARIL 13-V1KC Mineral Filled Polyphenylene Oxide (PPOm) (UL94V-1)
(Unverified Data**) Description: Laril thermoplastics are polyphenylene oxide (PPOm) products. They exhibit excellent toughness, even at low temperatures, good thermal resistance and dimensional stability are the most .. |
|||
Charpy Impact Unnotched | 1.10 J/cm² @Temperature -40.0 °C |
5.24 ft-lb/in² @Temperature -40.0 °F |
DIN 53453 |
LATI LARIL 13-V1KC Mineral Filled Polyphenylene Oxide (PPOm) (UL94V-1)
(Unverified Data**) Description: Laril thermoplastics are polyphenylene oxide (PPOm) products. They exhibit excellent toughness, even at low temperatures, good thermal resistance and dimensional stability are the most .. |
|||
Charpy Impact Unnotched | 1.10 J/cm² @Temperature 23.0 °C |
5.24 ft-lb/in² @Temperature 73.4 °F |
DIN 53453 |
LATI LARIL 13-V1KC Mineral Filled Polyphenylene Oxide (PPOm) (UL94V-1)
(Unverified Data**) Description: Laril thermoplastics are polyphenylene oxide (PPOm) products. They exhibit excellent toughness, even at low temperatures, good thermal resistance and dimensional stability are the most .. |
|||
Charpy Impact Unnotched | 1.10 J/cm² @Temperature -30.0 °C |
5.24 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
Inno-Comp INNOPOL® CS 1-2140 BLH 40% Talc-Filled Polypropylene Homopolymer INNOPOL® CS 1-2140 BLH is recommended especially for producing products, where high stiffness, low shrinkage, long term heat stability and excellent processability are required.All information pr.. |
|||
Charpy Impact Unnotched | 1.10 J/cm² @Temperature -20.0 °C |
5.23 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eA |
Borealis HK060AE Polypropylene Homopolymer HK060AE is a special low viscosity polypropylene homopolymer compound developed to fit the production of glass matt reinforced thermoplastics. This material is also suitable as base resin for the pr.. |
|||
Charpy Impact Unnotched | 1.10 J/cm² @Temperature -20.0 °C |
5.23 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eU |
Borealis MD441U Polypropylene Compound, Mineral Filled MD441U is a 40% mineral filled polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties and a medium melt flow rate. Applications: air cond.. |