Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 4.83 MPa

@Strain 300 %
700 psi

@Strain 300 %
ASTM D412
Teknor Apex Monprene® MP 1049 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Tensile Stress 4.83 MPa

@Strain 300 %
700 psi

@Strain 300 %
ASTM D412
Teknor Apex Monprene® MP-1451L Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Tensile Stress 4.83 MPa

@Strain 300 %
700 psi

@Strain 300 %
ASTM D412
Teknor Apex Monprene® MP-1488A Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Tensile Stress 4.83 MPa

@Strain 300 %
700 psi

@Strain 300 %
ASTM D412
Teknor Apex Monprene® MP-1531 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Tensile Stress 4.83 MPa

@Strain 300 %
700 psi

@Strain 300 %
ASTM D412
Teknor Apex Monprene® MP-1578 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Tensile Stress 4.83 MPa

@Strain 300 %
700 psi

@Strain 300 %
ASTM D412
Teknor Apex Monprene® MP-1671 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Tensile Stress 4.83 MPa

@Strain 300 %
700 psi

@Strain 300 %
ASTM D412
Teknor Apex Monprene® MP-2212A Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Tensile Stress 4.83 MPa

@Strain 300 %
700 psi

@Strain 300 %
ASTM D412
Teknor Apex Monprene® MP-2264B Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Tensile Stress 4.83 MPa

@Strain 300 %
700 psi

@Strain 300 %
ASTM D412
Teknor Apex Monprene® MP-2264R Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Tensile Stress 4.83 MPa

@Strain 300 %
700 psi

@Strain 300 %
ASTM D412
Teknor Apex Monprene® MP-2318 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Tensile Stress 4.83 MPa

@Strain 300 %
700 psi

@Strain 300 %
ASTM D412
Teknor Apex Monprene® MP-2357-A Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Tensile Stress 4.83 MPa

@Strain 100 %
700 psi

@Strain 100 %
ASTM D412
Teknor Apex Uniprene® UN-7010-80NT Thermoplastic Vulcanizate
Notes: Injection Rate: Fast Uses: Gaskets; Glazing; Grommets; Medical Pump Seals; Medical/Healthcare Applications; Plugs; Shock Absorbing Pads; Tubing Agency Ratings: NSF 61 Forms: Pellets Processin..