Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 23.0 MPa @Strain 100 % |
3340 psi @Strain 100 % |
|
AorTech Biomaterials Elast-Eon™ E2-860 Biomedical Polyurethane Pellets Elast-Eon™ 2-860 is a polyurethane with a 60% hard segment content and a mixed polyether/siloxane soft segment. It comes in pellet form. The pellets are colorless to yellowish and are soluble in DM.. |
|||
Tensile Stress | 23.0 MPa @Strain 100 % |
3340 psi @Strain 100 % |
|
AorTech Biomaterials Elast-Eon™ E2-860 Biomedical Polyurethane Pellets Elast-Eon™ 2-860 is a polyurethane with a 60% hard segment content and a mixed polyether/siloxane soft segment. It comes in pellet form. The pellets are colorless to yellowish and are soluble in DM.. |