Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 1.70 MPa @Strain 100 % |
247 psi @Strain 100 % |
ASTM D412 and ISO 37 |
ExxonMobil Exact™ 9061 Ethylene-based Plastomer Resin Product Description: Exact 9061 plastomer is an ethylene butene copolymer produced using ExxonMobil Chemical's EXXPOL™ Technology, exhibiting both plastic and elastomeric properties.Key Features:P.. |
|||
Tensile Stress | 1.70 MPa @Strain 100 % |
247 psi @Strain 100 % |
Across Flow; ASTM D412 |
ExxonMobil Santoprene® 121-50E500 Thermoplastic Elastomer A soft, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material has controlled rheology for robotic or specialty extrusion applications. This g.. |