Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 3.79 MPa @Strain 100 % |
550 psi @Strain 100 % |
510 mm/min; ASTM D412A |
PolyOne Geon™ Vinyl Flexible 86280 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Stress | 3.79 MPa @Strain 300 % |
550 psi @Strain 300 % |
ASTM D412 |
Teknor Apex Monprene® MP-1658A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Stress | 3.79 MPa @Strain 300 % |
550 psi @Strain 300 % |
ASTM D412 |
Teknor Apex Monprene® MP-1766 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Stress | 3.79 MPa @Strain 300 % |
550 psi @Strain 300 % |
ASTM D412 |
Teknor Apex Monprene® MP-1426A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |