Polymer Property : Tensile Strength at Break = 107500 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 741.2 MPa
107500 psi
0.76 lb. load and 0.003 in. diameter
Shakespeare WonderThread® SN-38 High tenacity TEX# 5 Nylon Industrial Sewing Thread
Used for sewing: Bedspreads, Comforters, Caps, Hats, Blankets, Stuffed Toys, Pillows, Carpets and Rugs, Handbags, Indoor Furniture, Curtains and Drapes, Apparel, Sleeping BagsInformation provided b..