Mechanical Properties Metric English Comments
Tensile Strength at Break 214 - 228 MPa
31000 - 33000 psi
Copper butt joint
Lucas-Milhaupt BRAZE 380
Characteristics:Braze 380 is a free-flowing, low temperature filler metal with excellent wetting of most ferrous and non-ferrous base metals, and is a good substitute for cadmium-bearing filler meta..
Tensile Strength at Break 193 - 228 MPa
28000 - 33000 psi
Copper butt joint
Lucas-Milhaupt BRAZE 452
Characteristics:Braze 452 is a free-flowing, low temperature filler metal commonly used to replace cadmium-bearing filler metals of similar silver content. This alloy is best suited for narrow gap ..
Tensile Strength at Break 207 - 228 MPa
30000 - 33000 psi
Copper butt joint
Lucas-Milhaupt BRAZE 700 (Medium) Silver Based Cadmium Free Filler Metal
Characteristics: This alloy is a intermediate silver brazing filler metals with a slight tendency to liquate (i.e. separate into low and high melting constituents) if heated slowly through their mel..
Tensile Strength at Break 179 - 228 MPa
26000 - 33000 psi
Strip, Temper-1/4 Hard
Lucas-Milhaupt BRAZE 999 Commercial Grade Fine Silver
Commercial grade fine silver (99.90% minimum silver) is widely used in numerous electrical, electronic, and industrial applications, such as contacts, fuse elements, lead wires, battery plated, and ..
Tensile Strength at Break 193 - 228 MPa
28000 - 33000 psi
Copper butt joint
Lucas-Milhaupt BRAZE 402 Silver Based Cadmium Free Filler Metal
Characteristics: Braze 402 is a free-flowing, intermediate temperature filler metal and as such is a good substitute for cadmium-bearing filler metals with similar silver contents. The material is ..