Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 19.0 - 22.0 MPa | 2760 - 3190 psi | ASTM D638 |
Daikin NEOFLON NP-101 FEP Pellets NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding.Applications: High speed wire and cable coatings.Information pro.. |
|||
Tensile Strength at Break | 19.0 - 22.0 MPa | 2760 - 3190 psi | ASTM D638 |
Daikin NEOFLON NP-120 FEP Pellets NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding.Applications: Heavy wall wire insulation, cable jacketing, tubes.. |
|||
Tensile Strength at Break | 19.0 - 22.0 MPa | 2760 - 3190 psi | ASTM D638 |
Daikin NEOFLON NP-130 FEP Pellets NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion.Applications: Heavy wall wire insulation, cable jacketing, pipe, shrinka.. |
|||
Tensile Strength at Break | 19.0 - 22.0 MPa | 2760 - 3190 psi | ASTM D638 |
Daikin NEOFLON NP-21 FEP Pellets NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding, injection molding.Applications: Suited to high speed extrusion .. |
|||
Tensile Strength at Break | 19.0 - 22.0 MPa | 2760 - 3190 psi | ASTM D638 |
Daikin NEOFLON NP-30 FEP Pellets NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding.Applications: Heavy wall wire insulation, tubes, cable jacketing.. |
|||
Tensile Strength at Break | 19.0 - 22.0 MPa | 2760 - 3190 psi | ASTM D638 |
Daikin NEOFLON NP-40 FEP Pellets NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding, transfer molding, compression molding.Applications: Films and s.. |
|||
Tensile Strength at Break | 19.0 - 22.0 MPa | 2760 - 3190 psi | ASTM D638 |
Daikin NEOFLON NP-20 FEP Pellets NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding, injection molding.Applications: Wire and cable coatings, films,.. |
|||
Tensile Strength at Break | 19.0 - 22.0 MPa | 2760 - 3190 psi | ASTM D638 |
Daikin NEOFLON NP-3000 FEP Pellets NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion.Applications: Ultra high speed wire and cable coatings.Information provi.. |