Tensile Strength at Break 6.76 MPa

@Temperature 23.0 °C
980 psi

@Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Dynaflex™ G7980-9 NSFG Thermoplastic Elastomer (TPE)
Dynaflex™ G7980-9 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. -NSF 51 approved -FDA (see Notes) -Overmold Adhesion to Polypropylene -Soft Touch,..
Tensile Strength at Break 6.76 MPa

@Temperature 23.0 °C
980 psi

@Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Dynaflex™ G7980-9001-02 Thermoplastic Elastomer (TPE)
Dynaflex™ G7980-9001-02 is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropylen..
Tensile Strength at Break 6.76 MPa

@Temperature 23.0 °C
980 psi

@Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Dynaflex™ G7980-1 NSFG Thermoplastic Elastomer (TPE)
Dynaflex™ G7980-1 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. -NSF 51 approved -FDA (see Notes) -Overmold Adhesion to Polypropylene -Soft Touch,..
Tensile Strength at Break 6.76 MPa

@Temperature 23.0 °C
980 psi

@Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Dynaflex™ G7980-1001-00 Thermoplastic Elastomer (TPE)
Dynaflex™ processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropylene - Rubbery Feel - Soft T..
Tensile Strength at Break >= 6.76 MPa
>= 980 psi
ASTM D412 Method A
Seals Eastern 5484 Nitrile Rubber
Low temperature service NitrileInformation provided by Seals Eastern, Inc.
Tensile Strength at Break 6.76 MPa

@Time 7200 sec
980 psi

@Time 2.00 hour
Die C; ASTM D414
STAR Thermoplastic Alloys & Rubbers StarTUFF TF 40-HR-9 TPE
Product Description: StarTUFF TF 40-HR-9 is an easy processing TPE designed for injection molding Features:Soft TouchRubbery FeelHigh Tear strengthHigh Tensile strengthProcessing Method: Injection M..
Tensile Strength at Break 6.76 MPa
980 psi
ASTM D412
Teknor Apex Telcar® TL-6800-73 Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Tensile Strength at Break 6.76 MPa
980 psi
ASTM D412
Teknor Apex Telcar® TL-93-T0488P-83 Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Tensile Strength at Break 6.76 MPa
980 psi
ASTM D412
Teknor Apex Uniprene® 73A Polyvinyl Chloride, Flexible
Features: High Elastic RecoveryInformation Provided by Teknor Apex