Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 6.58 MPa @Temperature 23.0 °C |
954 psi @Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Versollan™ OM 1255NX-1 Thermoplastic Elastomer (TPE) Versollan™ OM 1255NX-1 is a high performance TPU alloy designed for thin-wall overmolding onto polycarbonate (PC), ABS, PC/ABS and copolyester substrates. - Improved Grip with Matte, Rubbery Finish.. |
|||
Tensile Strength at Break | 6.58 MPa @Temperature 23.0 °C |
954 psi @Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Versollan™ OM 1255NX-9 Thermoplastic Elastomer (TPE) Versollan™ OM 1255NX-9 is a performance TPU alloy designed for thin wall overmolding onto polycarbonate (PC), ABS and PC/ABS substrates. - Improved Grip with Matte, Rubbery Finish - Superior Adhesi.. |
|||
Tensile Strength at Break | 6.58 MPa @Temperature 23.0 °C |
954 psi @Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Dynaflex™ G7970-9 NSFG Thermoplastic Elastomer (TPE) Dynaflex™ G7970-9 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. -NSF 51 approved -FDA (see Notes) -Overmold Adhesion to Polypropylene -Soft Touch,.. |
|||
Tensile Strength at Break | 6.58 MPa @Temperature 23.0 °C |
954 psi @Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Dynaflex™ G7970-1 NSFG Thermoplastic Elastomer (TPE) Dynaflex™ G7970-1 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. -NSF 51 approved -FDA (see Notes) -Overmold Adhesion to Polypropylene -Soft Touch,.. |
|||
Tensile Strength at Break | 6.58 MPa @Temperature 23.0 °C |
954 psi @Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Dynaflex™ G7970-1001-00 Thermoplastic Elastomer (TPE) Dynaflex™ G7970-1001-00 is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropylen.. |
|||
Tensile Strength at Break | 6.58 MPa @Temperature 23.0 °C |
954 psi @Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Dynaflex™ G7970-9001-02 Thermoplastic Elastomer (TPE) Dynaflex™ G7970-9001-02 is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropylen.. |
|||
Tensile Strength at Break | 6.58 MPa @Treatment Temp. 121 °C, Time 64800 sec |
954 psi @Treatment Temp. 250 °F, Time 18.0 hour |
in ASTM #2 Oil |
DuPont Elvax® 40L-03 High Temperature Ignition Cable Jacket Formulation
(discontinued **) Elvax® 40L-03 high temperature ignition cable jacket.Information provided by DuPont. |
|||
Tensile Strength at Break | 6.58 MPa @Treatment Temp. 121 °C, Time 64800 sec |
954 psi @Treatment Temp. 250 °F, Time 18.0 hour |
in ASTM #2 Oil |
DuPont Elvax® 40L-08 High Temperature Ignition Cable Jacket Formulation
(discontinued **) Elvax® 40L-08 high temperature ignition cable jacket.Information provided by DuPont. |
|||
Tensile Strength at Break | 6.58 MPa @Time 7200 sec |
954 psi @Time 2.00 hour |
Die C; ASTM D414 |
STAR Thermoplastic Alloys & Rubbers StarFlex® P 7380-9000 TPE Product Description: StarFlex P 7380-9000 is an easy processing TPE designed for injection molding Features:Soft TouchRubbery FeelGood WeatherabilityFDA and medical grades availableProcessing Method.. |