Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 6.55 MPa | 950 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible R5145B Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength at Break | 6.55 MPa | 950 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible R5145A Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength at Break | 6.55 MPa | 950 psi | 510 mm/min; ASTM D412A |
PolyOne Synprene® RT-3880M Styrene Butadiene Block Copolymer (SBC)
(discontinued **) Synprene™ thermoplastic elastomers (TPEs) are compounds based on styrenic block copolymer (SBC) technology, and can be formulated to deliver extremely low hardness values not found in other elastom.. |
|||
Tensile Strength at Break | 6.55 MPa | 950 psi | 0.010" Thick |
GrafTech GRAFOIL® GRAFKOTE® Laminates, Non-Metal Reinforced GRAFOIL® GRAFKOTE® laminates are made with GRAFOIL® Grade GTB flexible graphite thermally bonded to a 0.0005" thick polymer facing on one ("Single-Sided") or both ("Double-Sided") sides. Th.. |
|||
Tensile Strength at Break | 6.55 MPa | 950 psi | DBPH Cure |
Shin-Etsu Silicones SV-14000U Silicone Rubber SV14000U is one of a series of easy processing, no post cure silicone rubber bases. It can be used in a variety of applications requiring finishing by molding, extruding or calendering. Product Feat.. |
|||
Tensile Strength at Break | 6.55 MPa | 950 psi | ASTM D412 |
Teknor Apex Monprene® MP-1881E Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 6.55 MPa | 950 psi | ASTM D412 |
Teknor Apex Monprene® MP-2287C Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 6.55 MPa | 950 psi | ASTM D412 |
Teknor Apex Monprene® MP-2359A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 6.55 MPa | 950 psi | ASTM D412 |
Teknor Apex Monprene® MP-2664A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 6.55 MPa | 950 psi | ASTM D412 |
Teknor Apex Monprene® MP-2664B Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 6.55 MPa | 950 psi | ASTM D412 |
Teknor Apex Telcar® TL-1420A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Tensile Strength at Break | 6.55 MPa | 950 psi | ASTM D412 |
Teknor Apex Telcar® TL-1488G Thermoplastic Elastomer Uses: Flexible Grips; General Purpose; Handles; Household Goods; Safety Equipment; Toys Forms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Injection Rate: Moderate-Fast .. |
|||
Tensile Strength at Break | 6.55 MPa | 950 psi | ASTM D412 |
Teknor Apex Telcar® TL-2318G Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Tensile Strength at Break | 6.55 MPa | 950 psi | ASTM D412 |
Teknor Apex Telcar® TL-2535A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Tensile Strength at Break | 6.55 MPa | 950 psi | ASTM D412 |
Teknor Apex Telcar® TL-2550F Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Tensile Strength at Break | 6.55 MPa | 950 psi | ASTM D412 |
Teknor Apex Telcar® TL-2565A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Tensile Strength at Break | 6.55 MPa | 950 psi | ASTM D412 |
Teknor Apex Uniprene® UN-7200-73 Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Automotive Specifications: Chrysler MS-AK91; FORD WSS-M2D510-A7; .. |
|||
Tensile Strength at Break | 6.55 MPa | 950 psi | ASTM D412 |
Teknor Apex Telcar® TL-2470A Thermoplastic Elastomer Uses: Consumer Applications; Flexible Grips; General Purpose; Handles; Safety Equipment; Toys Forms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Injection Rate: Moderat.. |
|||
Tensile Strength at Break | 6.55 MPa | 950 psi | AFERA 4004 |
3M Scotch® 8347 Carry Handle Tape 3M™ Carry Handle Tape 8347 is a high-performance tape featuring a durable 3M™ Scotchpro™ Film backing that is longitudinal direction and an aggressive rubber resin adhesive especially suited for .. |
|||
Tensile Strength at Break | 6.55 MPa | 950 psi | ASTM D412 |
Teknor Apex Monprene® MP-2676B Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 6.55 MPa | 950 psi | TM R050-36 |
Resinlab® SEC1222 Silver Filled Epoxy Adhesive Resinlab™ SEC1222 is a silver filled, two component, room temperature curing epoxy adhesive. It is designed to cure completely at room temperature. SEC1222 provides excellent electrical conductivit.. |