Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 5.86 MPa | 850 psi | 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible D7000 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength at Break | 5.86 MPa | 850 psi | ASTM D412 |
Teknor Apex Monprene® MP-1775B Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 5.86 MPa | 850 psi | ASTM D412 |
Teknor Apex Monprene® MP-1775D Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 5.86 MPa | 850 psi | ASTM D412 |
Teknor Apex Monprene® MP-2228 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 5.86 MPa | 850 psi | ASTM D412 |
Teknor Apex Monprene® MP-2290A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 5.86 MPa | 850 psi | |
Shin-Etsu Silicones KE-1300T Silicone, Mold Making RTV Information Provided by Shin-Etsu Silicones of America, Inc. |
|||
Tensile Strength at Break | 5.86 MPa | 850 psi | |
Shin-Etsu Silicones KE-1310ST Silicone, Mold Making RTV Information Provided by Shin-Etsu Silicones of America, Inc. |
|||
Tensile Strength at Break | 5.86 MPa | 850 psi | |
Shin-Etsu Silicones KE-1311T Silicone, Mold Making RTV Information Provided by Shin-Etsu Silicones of America, Inc. |
|||
Tensile Strength at Break | 5.86 MPa | 850 psi | |
Shin-Etsu Silicones KE-5570U Low Temperature Silicone Elastomer ShinEtsu KE5570 U is a nominal 70 Durometer phenyl (PVMQ) base.Product Features: This material was designed for its excellent vibration dampening characteristics. Because of its phenyl content, it a.. |
|||
Tensile Strength at Break | 5.86 MPa | 850 psi | ASTM D412 |
Teknor Apex Monprene® MP 1213A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 5.86 MPa | 850 psi | ASTM D412 |
Teknor Apex Telcar® TL-1025-72 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; Closures; General Purpose; Grommets; Weatherstripping Forms:.. |
|||
Tensile Strength at Break | 5.86 MPa | 850 psi | ASTM D412 |
Teknor Apex Telcar® TL-1435A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Tensile Strength at Break | 5.86 MPa | 850 psi | ASTM D412 |
Teknor Apex Telcar® TL-2460A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Tensile Strength at Break | 5.86 MPa | 850 psi | ASTM D412 |
Teknor Apex Telcar® TL-2503S Thermoplastic Elastomer Uses: Consumer Applications; Flexible Grips; General Purpose; Handles; Safety Equipment; Toys Forms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Injection Rate: Moderat.. |
|||
Tensile Strength at Break | 5.86 MPa | 850 psi | ASTM D412 |
Teknor Apex Telcar® TL-3954-80 Thermoplastic Elastomer Uses: Appliance Wire Insulation; Appliance Wire Jacketing; Cable Jacketing; Connectors; Flexible Cord Jacketing; Industrial Cable Insulation; Terminal Cable Jacketing; Underground Power Cable; Wire .. |
|||
Tensile Strength at Break | 5.86 MPa | 850 psi | ASTM D638 |
ExxonMobil OPTEMA™ TC 120 Molding Ethylene Methyl Acrylate Product Description: Optema TC 120 is an ethylene methyl acrylate copolymer, which can be used as an impact modifier or compatibilizer in polymer compounds. TC 120 has been processed on typical LDPE.. |
|||
Tensile Strength at Break | 5.86 MPa | 850 psi | ASTM D638 |
ExxonMobil OPTEMA™ TC 220 Molding Ethylene Methyl Acrylate OPTEMA TC 220 is an ethylene methyl acrylate copolymer, which can be used in specialty bonding applications and as a toughener for engineering polymers. It can been processed at temperatures as low .. |
|||
Tensile Strength at Break | 5.86 MPa | 850 psi | Silicone Rubber Insulator; ASTM D412 |
3M 7620-S Cold Shrink QT-III Silicone Rubber Skirted Termination Kits 3M™ Cold Shrink QT-III Silicone Rubber Skirted Termination Kits, 7620-S, 7680-S and 7690-S Series, contain one-piece, skirted, silicone Rubber Skirted Terminations, qualified as IEEE Standard 48 Cl.. |
|||
Tensile Strength at Break | 5.86 MPa | 850 psi | Silicone Rubber Insulator; ASTM D412 |
3M 7620-T Cold Shrink Silicone Rubber Termination Kits QT-III 3M™ Cold Shrink QT-III Silicone Rubber Skirted Termination Kits, 7620-Tand 7690-T Series, contain one-piece, non-skirted, silicone rubber termination, qualified as IEEE Standard 48 Class 1 for indo.. |
|||
Tensile Strength at Break | 5.86 MPa | 850 psi | Silicone Rubber Insulator; ASTM D412 |
3M 7680-S Cold Shrink QT-III Silicone Rubber Skirted Termination Kits 3M™ Cold Shrink QT-III Silicone Rubber Skirted Termination Kits, 7620-S, 7680-S and 7690-S Series, contain one-piece, skirted, silicone Rubber Skirted Terminations, qualified as IEEE Standard 48 Cl.. |
|||
Tensile Strength at Break | 5.86 MPa | 850 psi | Silicone Rubber Insulator; ASTM D412 |
3M 7640-S Cold Shrink Silicone Rubber Termination Kits QT-III 3M™ Cold Shrink QT-III Silicone Rubber Skirted Termination Kits, 7640-S, 7650-S and 7660-S Series, contains one-piece, skirted, silicone rubber termination, qualified as IEEE Standard 48 Class 1 fo.. |
|||
Tensile Strength at Break | 5.86 MPa | 850 psi | Silicone Rubber Insulator; ASTM D412 |
3M 7650-S Cold Shrink Silicone Rubber Termination Kits QT-III 3M™ Cold Shrink QT-III Silicone Rubber Skirted Termination Kits, 7640-S, 7650-S and 7660-S Series, contains one-piece, skirted, silicone rubber termination, qualified as IEEE Standard 48 Class 1 fo.. |
|||
Tensile Strength at Break | 5.86 MPa | 850 psi | Silicone Rubber Insulator; ASTM D412 |
3M 7690-S Cold Shrink QT-III Silicone Rubber Skirted Termination Kits 3M™ Cold Shrink QT-III Silicone Rubber Skirted Termination Kits, 7620-S, 7680-S and 7690-S Series, contain one-piece, skirted, silicone Rubber Skirted Terminations, qualified as IEEE Standard 48 Cl.. |
|||
Tensile Strength at Break | 5.86 MPa | 850 psi | ASTM D412 |
Teknor Apex APEX® 3050-H Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Good FlexibilityUses-General Purpose, ProfilesAppearance-Natural Color, OpaqueForms-PelletsProcessin.. |