Mechanical Properties Metric English Comments
Tensile Strength at Break 47.6 MPa
6900 psi
chs 2 in/min; ASTM D638
Network Polymers NPS 80-1800 Crystal Polystyrene
Description: Injection Molding Grade, High Melt FlowInformation provided by Network Polymers Inc.
Tensile Strength at Break 47.6 MPa
6900 psi
Lucas-Milhaupt Silvabrite® 100® Lead-Free Solder
Silvabrite 100® was developed to meet market demands for a safe and easy to use solder for drinking water systems and other applications. Silvabrite 100® is a lead-free and antimony-free, non-..
Tensile Strength at Break 47.6 MPa
6900 psi
ASTM D 638
Shakespeare Isocorâ„¢ SC45BT Nylon 610
Isocorâ„¢ SC45BT is a medium viscosity PA-610 based copolymer. This resin is specifically suited for clear applications requiring increased solvent resistance and impact properties. Isocorâ„..
Tensile Strength at Break 47.6 MPa
6900 psi
94% Ret.
UBE UBESTA® 3030U Nylon 12 (After Sodium Hydroide for 500 hours)
Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c..
Tensile Strength at Break 47.6 MPa
6900 psi
94% Ret.
UBE UBESTA® 3030U Nylon 12 (After Sulfuric Acid (10%) for 1000 hours)
Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c..
Tensile Strength at Break 47.6 MPa
6900 psi
ASTM D638
Eastman Tenite 485E3720008 Cellulose Acetate Butyrate, Clear, Trsp
Applications:Toys/Sporting goodsProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties including toughness, hardness, strength, surface gloss, clarity,..
Tensile Strength at Break 47.6 MPa
6900 psi
ASTM D638
Americas Styrenics STYRON® 675 High Heat Crystal Polystyrene
Product CharacteristicsHigh heatMedium flowFood Contact CompliantUL Classification 94HBTypical ApplicationsThin-walled partsInformation provided by AmericasStyrenics LLC.
Tensile Strength at Break 47.6 MPa
6900 psi
50 mm/min; ASTM D638
Supreme Petrochem SP 6630 Antistatic Polystyrene
Characteristics Easy flow Excellent transparency Processing Extrusion Applications For glossy cap layer on HIPS To prevent dust patterns on thermoformed products Material Status: Commercial : Acti..