Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 44.8 MPa | 6500 psi | Mixed 1:1; TM R050-36 |
Resinlab® EP1215 Clear Unfilled Epoxy Structural Adhesive Resinlab™ EP1215 Clear is a two part unfilled epoxy structural adhesive designed for bonding applications requiring high strength and good impact resistance. It cures completely at room temperature.. |
|||
Tensile Strength at Break | 44.8 MPa | 6500 psi | TM R050-36 |
Resinlab® EP1390 Medium Viscosity, Self Extinguishing Flame Retardant Epoxy Casting Resin System Resinlab™ EP1390 is a RoHS compliant, medium viscosity, self extinguishing flame retardant epoxy casting resin system. It is recognized under the Component Recognition Program of Underwriters Labor.. |
|||
Tensile Strength at Break | 44.8 MPa | 6500 psi | ASTM D638 |
LNP Lubricomp® GFL-4034 EM M Polysulfone, Milled Glass Fiber Reinforcement, PTFE Lubricant
(discontinued **)& Features: Good Moldability, LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP g.. |
|||
Tensile Strength at Break | 44.8 MPa | 6500 psi | ASTM D412 |
Huntsman KRYSTALFLEX® PE 501 Polyurethane Optical Aliphatic Film Key Properties:Moisture ResistanceChemical CompatibilityCooler ProcessingHigher AdhesionMultiple Design OptionNo special storage requiredInformation provided by Alliance Polymers |
|||
Tensile Strength at Break | 44.8 MPa | 6500 psi | initial |
Malvern Minerals Nylon with Novakup® L-337 Silane-Treated Quartz Filler Product data demonstrates the effect of the Novakup® (lamellar quartz surface treated with A-1100) filler. A separate entry demonstrates the effect of untreated Novacite® filler in nylon. Th.. |
|||
Tensile Strength at Break | 44.8 MPa | 6500 psi | 89% Ret. |
UBE UBESTA® 3030U Nylon 12 (After Formic Acid (10%) for 500 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Tensile Strength at Break | 44.8 MPa | 6500 psi | ASTM D638 |
Chase Plastics CP Pryme® A300 BK General Purpose (Utility) ABS Molding Resin Information provided by Chase Plastics. |
|||
Tensile Strength at Break | 44.8 MPa | 6500 psi | at max load; ASTM D638 |
A. Schulman POLYFORT™ FPP 1244 Mineral Filled, General Purpose Polypropylene DescriptionPolyfort® FPP 1244 is a 40% mineral filled general purpose polypropylene for parts requiring ultra high stiffness, heat resistance and strength.Information provided by A. Schulman. |
|||
Tensile Strength at Break | 44.8 MPa | 6500 psi | ASTM D638 |
DuPont Surlyn® SG201U NC010 Supergloss Molding Alloy Surlyn® SG201U is a modified ionomer resin for applications that require a high gloss, molded in color surface color surface finish directly from the mold. The material is weatherable, durable, an.. |
|||
Tensile Strength at Break | 44.8 MPa | 6500 psi | at max load; ASTM D638 |
A. Schulman POLYFORT™ FPP 1244 Mineral Filled, General Purpose Polypropylene DescriptionPolyfort® FPP 1244 is a 40% mineral filled general purpose polypropylene for parts requiring ultra high stiffness, heat resistance and strength.Information provided by A. Schulman. |
|||
Tensile Strength at Break | 44.8 MPa | 6500 psi | at max load; ASTM D638 |
A. Schulman POLYFORT™ FPP 1244 Mineral Filled, General Purpose Polypropylene DescriptionPolyfort® FPP 1244 is a 40% mineral filled general purpose polypropylene for parts requiring ultra high stiffness, heat resistance and strength.Information provided by A. Schulman. |
|||
Tensile Strength at Break | 44.8 MPa | 6500 psi | TM R050-36 |
Resinlab® EP1026 Clear Epoxy Adhesive Resinlab™ EP1026 Clear is a two part unfilled epoxy adhesive designed for high speed bonding of metals, ceramics, and most plastics. It cures to a tough semi-rigid material, and is free flowing in .. |
|||
Tensile Strength at Break | 44.8 MPa | 6500 psi | ASTM D638 |
Resirene Resirene® HH-107 General Purpose Polystyrene Features:Medium FlowHigh HeatHigh Molecular WeightHigh ProductivityFDA Rating: 21 CFR 177.1640Mechanical StrengthApplications:Thin Wall ApplicationsExtrusionGPPS/HIPS BlendsCD CasesCassette CasesInf.. |
|||
Tensile Strength at Break | 44.8 MPa | 6500 psi | ASTM D638 |
Polymer Resources PPX-GP8 Modified PPO, General Purpose, Impact Modified
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Tensile Strength at Break | 44.8 MPa | 6500 psi | TM R050-36 |
Resinlab® EP1026 Black Epoxy Adhesive Resinlab™ EP1026 Black is a two part unfilled epoxy adhesive designed for high speed bonding of metals, ceramics, and most plastics. It cures to a tough semi-rigid material, and is free flowing in .. |