Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 35.9 MPa | 5210 psi | ASTM D638 |
Albis Plastics Cellulose Acetate Butyrate B902 (UV Inhibitor Added), 10% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Tensile Strength at Break | 35.9 MPa | 5210 psi | ASTM D638 |
Albis Plastics Cellulose Acetate Butyrate B9004 (Odor Mask Added), 10% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Tensile Strength at Break | 35.9 MPa | 5210 psi | ASTM D638 |
Albis Plastics Cellulose Acetate Butyrate B9024 (UVI, Odor Mask Added), 10% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Tensile Strength at Break | 35.9 MPa | 5210 psi | ASTM D638 |
Albis Plastics Cellulose Acetate Butyrate B9024 (UVI, Odor Mask Added), 10% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Tensile Strength at Break | 35.9 MPa | 5210 psi | ASTM D638 |
LNP Stat-Kon® PDX-S-90398 Polyamide 12, Stainless Steel Fiber
(discontinued **) Features: Electrically ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades.. |
|||
Tensile Strength at Break | 35.9 MPa | 5210 psi | ASTM D638 |
Resirene Resirene® HF-666 General Purpose Polystyrene Features:High FlowEasy ProcessingHigh ProductivityFDA Rating: 21 CFR 177.1640External Lubrication AvailableApplications:Medium Wall ApplicationsInjectionToysCassette CasesInformation provided by US .. |
|||
Tensile Strength at Break | 35.9 MPa | 5210 psi | ASTM D638 |
Albis Plastics Cellulose Acetate Butyrate B900 (Base Grade), 10% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Tensile Strength at Break | 35.9 MPa | 5210 psi | ASTM D638 |
Albis Plastics Cellulose Acetate Butyrate B900 (Base Grade), 10% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Tensile Strength at Break | 35.9 MPa | 5210 psi | ASTM D638 |
Albis Plastics Cellulose Acetate Butyrate B902 (UV Inhibitor Added), 10% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Tensile Strength at Break | 35.9 MPa | 5210 psi | ASTM D638 |
Albis Plastics Cellulose Acetate Butyrate B9004 (Odor Mask Added), 10% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Tensile Strength at Break | 35.9 MPa | 5210 psi | ASTM D638 |
Albis Plastics Cellulose Acetate Butyrate B9086 (FDA Odor Mask), 10% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |