Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 221 MPa | 32000 psi | ASTM D638 |
Polymer Resources NY6-G43 Nylon 6, 43% Glass Reinforced Nylon 6, 43% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are teste.. |
|||
Tensile Strength at Break | 221 MPa | 32000 psi | ASTM D638 |
Ravago Manufacturing Americas Hylon® N1043HL Nylon 6/6 (DAM) Information provided by Ravago. |
|||
Tensile Strength at Break | 221 MPa | 32000 psi | ASTM D638 |
Ravago Manufacturing Americas Hylon® N1043L Nylon 6/6 (DAM) Information provided by Ravago. |
|||
Tensile Strength at Break | 221 MPa | 32000 psi | ASTM D638 |
Polymer Resources NY6-G43-[color]-H Nylon 6, 43% Glass Reinforced, Heat Stabilized Nylon 6, 43% Glass Reinforced, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon.. |