Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 17.2 MPa | 2490 psi | 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible B5DU0 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength at Break | 17.2 MPa | 2490 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ HC 2175G Polyvinyl Chloride, Flexible (PVC, Flexible) Geon HC 2175G is a 75 Shore A non-phthalate, gamma-stable flexible vinyl compound made from FDA sanctioned ingredients. HC 2175G can be used for extrusion and injection molding healthcare applicatio.. |
|||
Tensile Strength at Break | 17.2 MPa | 2490 psi | 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible B9000 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength at Break | 17.2 MPa | 2490 psi | ASTM D3759 |
3M 3W55Z Protective UV Tape 3M™ Protective UV Tape 3W55X is a black and white co-extruded polyethylene tape for temporary indoor and outdoor protection of many metals, plastics and glass.Information provided by 3M |
|||
Tensile Strength at Break | 17.2 MPa | 2490 psi | ASTM D3759 |
3M 41825 Industrial Polyethylene Temporary Surface Protection Tape 3M™ Industrial Polyethylene Temporary Surface Protection Tape 41825 is a very low adhesion temporary protection tape designed for a variety of surface protection applications.Information provided b.. |
|||
Tensile Strength at Break | >= 17.2 MPa | >= 2490 psi | |
3M Controltac™ 8620 ES Conformable Graphic Film These 2 mil films offer versatility along with sideable, repositionable, pressure activated adhesive. These long term durable and removable films have excellent hiding power and stability, making th.. |
|||
Tensile Strength at Break | >= 17.2 MPa | >= 2490 psi | |
3M Controltac™ IJ3552C Changeable Graphic Film with Comply™ Adhesive 2-mil white, vinyl film; Pressure-activated adhesive for easy sliding, tacking, snap up and repositioning; Conformers to surface with corrugations and rivets; Air release channels for fast, easy, bu.. |
|||
Tensile Strength at Break | 17.2 MPa | 2490 psi | |
3M Scotchcal™ 1000-37 Graphic Film 2-mil vinyl film; Wide color selection; Includes three colors with both a layflat liner and gray adhesive for excellent hiding power and a transparent film with a layflat liner; Pressure-sensitive a.. |
|||
Tensile Strength at Break | 17.2 MPa | 2490 psi | |
3M Scotchcal™ 3632-53 Translucent Film 2-mil translucent cast vinyl film; Matte surface finish that eliminates glare and provides uniform color in reflective light; Built in Graphic Protection System (GPS), which is a top coat that incre.. |
|||
Tensile Strength at Break | 17.2 MPa | 2490 psi | |
3M Scotchcal™ ElectroCut™ 7125-13 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color.. |
|||
Tensile Strength at Break | 17.2 MPa | 2490 psi | |
3M Scotchcal™ ElectroCut™ 7125-177 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color.. |
|||
Tensile Strength at Break | 17.2 MPa | 2490 psi | |
3M Scotchcal™ ElectroCut™ 7125-187 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color.. |
|||
Tensile Strength at Break | 17.2 MPa | 2490 psi | |
3M Scotchcal™ ElectroCut™ 7125-23 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color.. |
|||
Tensile Strength at Break | 17.2 MPa | 2490 psi | |
3M Scotchcal™ ElectroCut™ 7125-37 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color.. |
|||
Tensile Strength at Break | 17.2 MPa | 2490 psi | |
3M Scotchcal™ ElectroCut™ 7125-47 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color.. |
|||
Tensile Strength at Break | 17.2 MPa | 2490 psi | |
3M Scotchcal™ ElectroCut™ 7125-77 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color.. |
|||
Tensile Strength at Break | 17.2 MPa | 2490 psi | |
3M Scotchcal™ ElectroCut™ 7125-85 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color.. |
|||
Tensile Strength at Break | 17.2 MPa | 2490 psi | |
3M Scotchcal™ ElectroCut™ 7125-89 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color.. |
|||
Tensile Strength at Break | 17.2 MPa | 2490 psi | |
3M Scotchcal™ ElectroCut™ 7125-90 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color.. |
|||
Tensile Strength at Break | 17.2 MPa | 2490 psi | |
3M Scotchcal™ ElectroCut™ 7725-15 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass.. |
|||
Tensile Strength at Break | 17.2 MPa | 2490 psi | |
3M Scotchcal™ ElectroCut™ 7725-193 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass.. |
|||
Tensile Strength at Break | >= 17.2 MPa | >= 2490 psi | |
3M Controltac™ 8620Cv3 ES Changeable Graphic Film with Comply™ v3 Adhesive These 2 mil films offer versatility along with sideable, repositionable, pressure activated adhesive. These long term durable and removable films have excellent hiding power and stability, making th.. |
|||
Tensile Strength at Break | 17.2 MPa | 2490 psi | |
3M Scotchcal™ 1000-131 Graphic Film 2-mil vinyl film; Wide color selection; Includes three colors with both a layflat liner and gray adhesive for excellent hiding power and a transparent film with a layflat liner; Pressure-sensitive a.. |
|||
Tensile Strength at Break | 17.2 MPa | 2490 psi | |
3M Scotchcal™ 1000-25 Graphic Film 2-mil vinyl film; Wide color selection; Includes three colors with both a layflat liner and gray adhesive for excellent hiding power and a transparent film with a layflat liner; Pressure-sensitive a.. |
|||
Tensile Strength at Break | 17.2 MPa | 2490 psi | |
3M Scotchcal™ 3632-126 Translucent Film 2-mil translucent cast vinyl film; Matte surface finish that eliminates glare and provides uniform color in reflective light; Built in Graphic Protection System (GPS), which is a top coat that incre.. |
|||
Tensile Strength at Break | 17.2 MPa | 2490 psi | |
3M Scotchcal™ ElectroCut™ 7725-29 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass.. |
|||
Tensile Strength at Break | 17.2 MPa | 2490 psi | |
3M Scotchcal™ 1000LF-12 Graphic Film 2-mil vinyl film; Wide color selection; Includes three colors with both a layflat liner and gray adhesive for excellent hiding power and a transparent film with a layflat liner; Pressure-sensitive a.. |
|||
Tensile Strength at Break | 17.2 MPa | 2490 psi | |
3M Scotchcal™ 3632-20 Translucent Film 2-mil translucent cast vinyl film; Matte surface finish that eliminates glare and provides uniform color in reflective light; Built in Graphic Protection System (GPS), which is a top coat that incre.. |
|||
Tensile Strength at Break | >= 17.2 MPa | >= 2490 psi | |
3M Scotchcal™ 8000-25 Graphic Film This 2-mil, screen printable film with a pressure sensitive adhesive that can be used on flat and simple curved surfaces. This film withstands severe weather dn handling conditions encountered by co.. |
|||
Tensile Strength at Break | 17.2 MPa | 2490 psi | 5mm/min; ASTM D638 |
Mitsui TPX® RT18 Methylpentene Copolymer, Transparent Grade TPX® is a 4-methylpentene-1 based polyolefin with a unique combination of transparency, heat and chemical resistant qualities. TPX is used in a wide variety of applications, including: medical equi.. |