Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 9.72 MPa | 1410 psi | 510 mm/min; ASTM D412A |
PolyOne Elastamax™ XL-2185 Thermoplastic Polyolefin Elastomer (TPO (POE)) PolyOne's Elastamax™ XL thermoplastic olefins (TPOs) are based on pelletized blends of polyolefin resins and select elastomers such EPDM. These materials have been engineered to provide a balance o.. |
|||
Tensile Strength at Break | 9.72 MPa | 1410 psi | Across Flow; ASTM D412 |
ExxonMobil Santoprene® 281-73MED Thermoplastic Elastomer
(discontinued **) A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of our medical grad.. |
|||
Tensile Strength at Break | 9.70 MPa | 1410 psi | 500 mm/min; ASTM D638 |
Eastman E6838-889P Polyethylene
(discontinued **) Polyethylene E6838-889P is a formulation suggested for extrusion coating applications and has been used successfully in compounding. This product may be used for holding food during cooking.Applicat.. |
|||
Tensile Strength at Break | 9.70 MPa | 1410 psi | |
GrafTech eGRAF® SPREADERSHIELD™ SS400 Graphite Made from flexible graphite, eGRAF® SPREADERSHIELD™ products function as both a passive heat spreader and heat shield. SPREADERSHIELD™ material can be die-cut, press-formed, or laminate.. |
|||
Tensile Strength at Break | 9.70 MPa | 1410 psi | |
GrafTech eGRAF® SPREADERSHIELD™ SS600 Graphite Made from flexible graphite, eGRAF® SPREADERSHIELD™ products function as both a passive heat spreader and heat shield. SPREADERSHIELD™ material can be die-cut, press-formed, or laminate.. |
|||
Tensile Strength at Break | 9.70 MPa | 1410 psi | 500mm/min; ASTM D638 Type IV Specimen |
Westlake EC850AA Low Density Polyethylene WESTLAKE low-density polyethylene EC850 is a resin designed for applications where high coating speeds and good drawdown are required. The combination of high melt index and low density provides goo.. |
|||
Tensile Strength at Break | 9.70 MPa | 1410 psi | 500mm/min; ASTM D638 Type IV Specimen |
Westlake EM1870AA Low Density Polyethylene WESTLAKE low-density polyethylene EM1870 is used for injection molding applications. It has excellent stress crack resistance for lids.Application/UsesFlexible medicalLidsMedicalFDA: This material c.. |
|||
Tensile Strength at Break | 9.70 MPa | 1410 psi | ISO 527-1 |
Barlog Plastics KEBAFLEX S 65 A.02 TPE-S, Shore A65, translucent TPE-SInformation provided by BARLOG plastics GmbH. |