Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 8.27 MPa | 1200 psi | 510 mm/min; ASTM D412A |
PolyOne Elastamax™ XL-2085 Thermoplastic Polyolefin Elastomer (TPO (POE)) PolyOne's Elastamax™ XL thermoplastic olefins (TPOs) are based on pelletized blends of polyolefin resins and select elastomers such EPDM. These materials have been engineered to provide a balance o.. |
|||
Tensile Strength at Break | 8.27 MPa @Temperature 23.0 °C |
1200 psi @Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Dynaflex™ G2780C Thermoplastic Elastomer (TPE) Dynaflex™ G2780C is an easy processing TPE designed for injection molding and extrusion applications that require FDA compliance. - Excellent Colorability - Good Ozone and UV Stability - Overmold A.. |
|||
Tensile Strength at Break | 8.27 MPa | 1200 psi | 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible C6502 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength at Break | 8.27 MPa | 1200 psi | ASTM D638 |
LyondellBasell Petrothene® GA564189 Linear Low Density Polyethylene, Injection Molding Grade PETROTHENE GA564189 exhibits good stiffness and low temperature toughness. Typical applications include trash cans, industrial containers, housewares and toys. Regulatory Status: GA564189 meets the .. |
|||
Tensile Strength at Break | 8.27 MPa | 1200 psi | ASTM D412 |
Teknor Apex Monprene® MP 1871R Thermoplastic Elastomer Notes: USP Class VI; ISO 10993; Clear Features: Good Stability Uses: Medical TubingInformation Provided by Teknor Apex |
|||
Tensile Strength at Break | 8.27 MPa | 1200 psi | ASTM D412 |
Teknor Apex Monprene® MP 7002 Thermoplastic Elastomer Notes: Semi-transparent Features: Good Chemical and Oil ResistanceInformation Provided by Teknor Apex |
|||
Tensile Strength at Break | 8.27 MPa | 1200 psi | ASTM D412 |
Teknor Apex Monprene® MP-1579D Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 8.27 MPa | 1200 psi | ASTM D412 |
Teknor Apex Monprene® MP-1580-L3 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 8.27 MPa | 1200 psi | ASTM D412 |
Teknor Apex Monprene® MP-1665-L3 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 8.27 MPa | 1200 psi | ASTM D412 |
Teknor Apex Monprene® MP-1890UV Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 8.27 MPa | 1200 psi | ASTM D412 |
Teknor Apex Monprene® MP 1595 Thermoplastic Elastomer Features: Nice Silken Feel Uses: Leisure ProductsInformation Provided by Teknor Apex |
|||
Tensile Strength at Break | 8.27 MPa | 1200 psi | ASTM D412 |
Teknor Apex Telcar® TL EF-6155 UV Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Tensile Strength at Break | 8.27 MPa | 1200 psi | ASTM D412 |
Teknor Apex Telcar® TL-1025-85 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Tensile Strength at Break | 8.27 MPa | 1200 psi | ASTM D412 |
Teknor Apex Telcar® TL-1536D Thermoplastic Elastomer Uses: Consumer Applications; General Purpose; Household Goods; Food Containers; Handles; Lids Forms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Injection Rate: Moderat.. |
|||
Tensile Strength at Break | 8.27 MPa | 1200 psi | ASTM D412 |
Teknor Apex Telcar® TL-87-L832A Thermoplastic Elastomer Notes: UV Stabilized Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstrip.. |
|||
Tensile Strength at Break | 8.30 MPa | 1200 psi | 500mm/min; ASTM D638 Type IV Specimen |
Westlake EC4056AA Low Density Polyethylene WESTLAKE low-density polyethylene EC4056 is a natural low density material with an 80 melt index.FDA: This material complies with FDA regulations in 21 CFR, section 177.1520. Kosher Compliant.All in.. |
|||
Tensile Strength at Break | 8.27 MPa | 1200 psi | 500 mm/min (20 in./min); ASTM-D638 Type IV Specimen |
Westlake EMAC® SP2409 20% EMA Copolymer Westlake EMAC� SP2409 is a 20% EMA copolymer designed for extrusion coating, tie-layers, and extrusions where flexibility, compatibility, low heat seal temperatures, or a high coefficient of fr.. |
|||
Tensile Strength at Break | 8.27 MPa | 1200 psi | ASTM D412 |
Teknor Apex Uniprene® UN-7100-80 Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
Tensile Strength at Break | 8.27 MPa | 1200 psi | ASTM D638 |
ExxonMobil Escorene™ UL 7760 Ethylene Vinyl Acetate Copolymer Product Description: Escorene Ultra UL 7760 is a high viscosity, 26.7% VA copolymer that has very good flexibility and low temperature toughness. It has good compatibility with both hydrocarbon and .. |
|||
Tensile Strength at Break | 8.30 MPa | 1200 psi | Across Flow; ASTM D412 and ISO 37 |
ExxonMobil Santoprene® 691-73W175 Thermoplastic Vulcanizate Product Description: A soft, colorable thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material is designed for thin wall, architectural glazing and sealing applic.. |
|||
Tensile Strength at Break | 8.27 MPa | 1200 psi | Molded and tested in accordance with ASTM D4976; ASTM D638 |
Dow DNDB-1077 NT 7 Linear Low Density Polyethylene Resin DOW DNDB-1077 NT 7 is produced using UNIPOL™ PE process technology. It is intended for high-speed injection molding of thin walled parts such as downguaged lids. Information provided by Dow |
|||
Tensile Strength at Break | 8.27 MPa | 1200 psi | ASTM D412 |
Teknor Apex Monprene® MP 1245A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |