Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | <= 7.80 MPa | <= 1130 psi | ISO/R527 |
Polykemi AB POLYelast TPE Z606 Thermoplastic Elastomer, SEBS-based Information provided by Polykemi AB |
|||
Tensile Strength at Break | 7.79 MPa | 1130 psi | ASTM D412 |
Teknor Apex Monprene® MP-1358C Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 7.79 MPa | 1130 psi | ASTM D412 |
Teknor Apex Telcar® TL-3954-90 Thermoplastic Elastomer Uses: Appliance Wire Insulation; Appliance Wire Jacketing; Cable Jacketing; Connectors; Flexible Cord Jacketing; Industrial Cable Insulation; Terminal Cable Jacketing; Underground Power Cable; Wire .. |
|||
Tensile Strength at Break | 7.76 MPa | 1130 psi | Longitudinal; ASTM D3759 |
3M ScotchPad™ 3750P Tape Pad 3M™ ScotchPad™ Tape Pad 3750P is a pre-cut pad formed with layered, high-performance tape sheets featuring durable 3M™Scotchpro™ film backing that is strong, conformable, and resistant to impact.. |
|||
Tensile Strength at Break | 7.76 MPa | 1130 psi | Longitudinal; ASTM D3759 |
3M ScotchPad™ 809G Custom Tape Pads 3M™ ScotchPad™ Custom Tape Pad 809G is a pre-cut pad formed with layered, high performance tape sheets featuring durable 3M™ Scotchpro™ film backing that is strong, conformable and resistant to .. |
|||
Tensile Strength at Break | 7.76 MPa | 1130 psi | Longitudinal; ASTM D3759 |
3M ScotchPad™ 822 Label Protection Tape Pad 3M™ ScotchPad™ Label Protection Tape Pad 822 is a pre-cut pad formed with layered high-performance tape sheets featuring durable 3M™ ScotchPad™ polypropylene film backing that is strong, conform.. |