Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 7.64 MPa @Temperature 23.0 °C |
1110 psi @Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Versollan™ OM 1262NX-1 Thermoplastic Elastomer (TPE) Versollan™ OM 1262NX-1 is a performance TPU alloy designed for thin-wall overmolding onto polycarbonate (PC), ABS and PC/ABS substrates. - Excellent Grip with Matte, Rubbery Finish - Proven Track R.. |
|||
Tensile Strength at Break | 7.64 MPa @Temperature 23.0 °C |
1110 psi @Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Versollan™ OM 1262NX-9 Thermoplastic Elastomer (TPE) Versollan™ OM 1262NX-9 is a performance TPU alloy designed for thin-wall overmolding onto polycarbonate (PC), ABS, PC/ABS and copolyester substrates. - Excellent Grip with Matte, Rubbery Finish - P.. |
|||
Tensile Strength at Break | 7.65 MPa | 1110 psi | 510 mm/min; ASTM D412A |
PolyOne Elastamax™ XL-0153-56 Styrene Butadiene Block Copolymer (SBC)
(discontinued **) A thermoplastic elastomer compound formulated for use in food contact applications. The physical properties listed above are typical values obtained on laboratory prepared samples and tested in acco.. |