Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 6.998 MPa | 1015 psi | |
Aearo E-A-R Specialty Composites Isoloss® HDF Polyurethane Elastomer Isoloss® Polyurethane Elastomers feature high internal damping properties for low amplification at resonance to protect equipment during frequency cycling and random shocks, effective shock protect.. |