Aearo E-A-R Specialty Composites Isoloss® HDF Polyurethane Elastomer

Category Polymer , Thermoset , Polyurethane, TS , Thermoset Polyurethane, Elastomer, Unreinforced , Rubber or Thermoset Elastomer (TSE)
Manufacturer Aearo E-A-R Specialty Composites
Trade Name Isoloss®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aearo E-A-R Specialty Composites Isoloss® HDF Polyurethane Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Isoloss® Polyurethane Elastomers feature high internal damping properties for low amplification at resonance to protect equipment during frequency cycling and random shocks, effective shock protection for sensitive mechanisms within minimum sway parameters, and quick return to equilibrium after vibrations or shocks.Information provided by Aearo E-A-R Specialty Composites.
Mechanical Properties Metric English Comments
Hardness, Shore A 56
56
Tensile Strength at Break 6.998 MPa
1015 psi
Elongation at Break 424 %
424 %
Resilience 4.5
4.5
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 82.0 °C
180 °F
Brittleness Temperature -27.0 °C
-16.6 °F
Flammability, UL94 V-2
V-2
Descriptive Properties Value Comments
Abrasion Resistance Excellent
Compression Set Resistance Excellent
Damping T max 4 dB
Heat Aging; 100°C Fair to Good
Tear Strength Excellent